Enhanced band-edge photoluminescence from ZnO-passivated ZnO nanoflowers by atomic layer deposition

The ZnO nanoflowers were synthesized by reactive vapor deposition. A secondary nucleation in the stalk/leaves interface was suggested. The photoluminescence revealed that there were many oxygen vacancies in the nanoflowers. To tune the optical properties of ZnO nanoflowers, ZnO thin films with varying thicknesses were coated on the nanoflowers by atomic layer deposition, which can distinctly im...

متن کامل

Enhanced visible photoluminescence from ultrathin ZnO films grown on Si-nanowires by atomic layer deposition.

Bright room temperature visible emission is obtained in heterostructures consisting of approximately 3.5 nm thick ZnO ultrathin films grown on Si-nanowires produced by means of self-masking dry etching in hydrogen-containing plasma. The ZnO films were deposited on Si-nanowires by using atomic layer deposition (ALD) under an ambient temperature of 25 degrees C. The orders of magnitude enhancemen...

متن کامل

Pd nanoparticles on ZnO-passivated porous carbon by atomic layer deposition: an effective electrochemical catalyst for Li-O2 battery.

Uniformly dispersed Pd nanoparticles on ZnO-passivated porous carbon were synthesized via an atomic layer deposition (ALD) technique, which was tested as a cathode material in a rechargeable Li-O2 battery, showing a highly active catalytic effect toward the electrochemical reactions-in particular, the oxygen evolution reaction. Transmission electron microscopy (TEM) showed discrete crystalline ...

متن کامل

Enhanced free exciton and direct band-edge emissions at room temperature in ultrathin ZnO films grown on Si nanopillars by atomic layer deposition.

Room-temperature ultraviolet (UV) luminescence was investigated for the atomic layer deposited ZnO films grown on silicon nanopillars (Si-NPs) fabricated by self-masking dry etching in hydrogen-containing plasma. For films deposited at 200 °C, an intensive UV emission corresponding to free-exciton recombination (~3.31 eV) was observed with a nearly complete suppression of the defect-associated ...

متن کامل

Improved characteristics of near-band-edge and deep-level emissions from ZnO nanorod arrays by atomic-layer-deposited Al2O3 and ZnO shell layers

We report on the characteristics of near-band-edge (NBE) emission and deep-level band from ZnO/Al2O3 and ZnO/ZnO core-shell nanorod arrays (NRAs). Vertically aligned ZnO NRAs were synthesized by an aqueous chemical method, and the Al2O3 and ZnO shell layers were prepared by the highly conformal atomic layer deposition technique. Photoluminescence measurements revealed that the deep-level band w...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Nanoscale Research Letters

سال: 2013

ISSN: 1556-276X

DOI: 10.1186/1556-276x-8-105