Electron microscopy study of laser welded GH909 superalloy joint

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Analysis of Cracks in the Pulsed Nd:YAG Laser Welded Joint of Nickel-Based Superalloy

The weldability of GTD-111 nickel-based superalloy by pulsed Nd:YAG laser welding with an average power of 250 W was studied, and the microstructural evolution and cracking characteristics were also investigated. The solidification cracking of the fusion zone (FZ) and the intergranular liquation cracking in the heat affected zone (HAZ) were observed in the joint. Solidification cracking was cau...

متن کامل

Transmission Electron Microscopy Sample Preparation of INCONEL 738 Nickel-Base Superalloy

Size, shape, volume fraction and distribution of embedded g/ phase in g phase has direct effect on strength of INCONEL alloy. Microstructure parameters of INCONEL phases are quantified from microstructure images using transmission electron microscopy (TEM). Different TEM sample preparation techniques were used to study INCONEL 738 alloy microstructure for transmission electron micros...

متن کامل

Defects characterization of welded specimens by transmission electron microscopy

Austenitic Type 304L stainless steel (SS) and martensitic Alloy EP-823 have been identified as candidate structural materials to contain spallation arget for transmutation of nuclear waste. Welded specimens consisting of either or both materials have been evaluated by transmission electron icroscopy (TEM) to determine the dislocation density near the heat-affected-zone (HAZ) and the base materi...

متن کامل

Examination of Lung Parenchyma by Electron Microscopy

In this paper many of the principal struc­ture of the Moral Lung were studied with the help of Electron Microscopy. Detailed descrip­tion was given of Granular Pneumocytes, Membranous Pneumocytes, Macrophages, and Alveolar Capillaries. A discussion followed on the form and function of Granular Pneumo­cytes.  Acknowledgements  I am grateful to the Reza Shah Pahlavi Foundation for its generou...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Materials Research and Technology

سال: 2020

ISSN: 2238-7854

DOI: 10.1016/j.jmrt.2020.10.049