Electrochemical and fractographic analysis of Microbiologically Assisted Stress Corrosion Cracking of carbon steel

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

ELECTROCHEMICAL NOISE ANALYSIS OF 70-30 BRASS DURING STRESS CORROSION CRACKING TEST IN MATTSON S SOLUTION

An investigation of the electrochemical noise generation during Stress Corrosion Cracking (SCC) of 70-30 Brass in Mattson's solution was conducted. The fluctuations of potential and current were monitored. The relationship between potential and current fluctuations has been evaluated in time domain and the obtained data has been analyzed in the frequency domain using Power Spectral Density (PSD...

متن کامل

Electrochemical Noise Analysis of Anaerobic (Bacterial) Corrosion of Steel

Corrosion of structural steel in an SRB containing environment for as long as 9 months, is studied using the Electrochemical Noise Analysis technique. The results show that the activity of the system, which was very low initially, started to increase after 6 months exposure to the environment. The power spectral density curves of the Electrochemical Potential Noise of the system, using the maxi...

متن کامل

Stress Corrosion Cracking Detection of Sensitized Stainless Steel 304 in Chloride Media by Using Electrochemical Impedance Spectroscopy (EIS)

Electrochemical impedance spectroscopy (EIS) was used to detect stress corrosion cracking (SCC) in stainless steel 304 alloy exposed to an aqueous environment at 120 °C. Stainless steel 304 alloy as u-bend was tested in the solution that contains 40 weight percent of magnesium chloride. U-bended samples were prepared according to ASTM G30. EIS measurements were always performed simultaneously o...

متن کامل

An Investigation on Corrosion and Stress Corrosion Cracking initiation of a Ferritic Stainless Steel in a Tertiary Amine Solution

The present study focused on stress corrosion cracking (SCC) and corrosion behavior of ferritic stainless steel (grade 430) in activated methyl diethanolamine (aMDEA) solution, which is classified as a tertiary amine. In this regard, cyclic polarization and U-bend tests were performed in CO2 loaded aMDEA with different concentrations at 25 and 70 °C to observe corrosion behavior and ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Corrosion Science

سال: 2014

ISSN: 0010-938X

DOI: 10.1016/j.corsci.2013.11.009