Abstract High-entropy alloy, a new generation material, exhibits superior structural properties. For high-temperature applications, where dissimilar materials are in demand, HEAs may be joined with commercially available to improve their performance-life ratio. In this connection, joint was fabricated by gas tungsten arc welding between Al 0.1 CoCrFeNi-HEA and Inconel 718. The columnar dendritic grains growing epitaxially at the CoCrFeNi-HEA/weld metal interface, compositions matching. While composition misfit weld metal/Inconel 718 reveals non-epitaxial mode of solidification. addition, fusion zone porosity micro-segregation NbC Laves phases. shows efficiency ~ 88%, strength is observed 644 MPa 21% ductility. results demonstrate applicability GTAW fabricating joints HEA for applications. Graphic abstract
منابع مشابه
Investigation of Cutting Forces Superalloy Inconel 718
Since the cutting tools used in machining process of super alloys are subjected to high cutting forces, accordingly tools life is reduced, therefore improvement in alloys machining and reducing cutting forces to achieve longer tools life is an essential necessity. In this research, the effect of changes in feed rate on cutting forces in machining process of nickel based super alloys is investig...
متن کاملCharacterization of strain induced precipitation in Inconel 718 superalloy
Inconel 718 is a Ni-Cr-Fe superalloy which presents excellent mechanical properties at high temperatures, as well as good corrosion resistance and weldability. These characteristics can be optimized with an appropriate control of microstructural features such as grain size and precipitation. Precipitates of different nature can form in these alloys, i.e. γ’’ (a metastable metallic compound Ni3N...
متن کاملEffect of Thermomechanical Working on the Microstructure and Mechanical Properties of Hot Pressed Superalloy Inconel 718
Experimental results on hot deformation and dynamic structural processes of nickel based alloy Inconel 718 are reviewed. The focus is the analysis of dynamic precipitation processes which operate during hot deformation of these materials at elevated temperatures. Hot compression tests were performed on the solution treated precipitation hardenable nickel based superalloy Inconel 718 at 720-1150...
متن کاملHigh temperature fatigue crack propagation behaviour of Inconel 718
The overall objective of this work has been to develop and evaluate tools for designing against fatigue in gas turbine applications, with special focus on the nickelbased superalloy Inconel 718. The fatigue crack propagation behaviour under high temperature hold times has been studied. Firstly, the main fatigue crack propagation phenomena have been investigated with the aim of setting up a basi...
متن کاملEvaluation of Tool Performance With Nanocrystalline Multilayer Coatings on the Machinability of Superalloy Inconel 718
In this paper, the performance of the cutting tool with nanocrystalline multilayer coatings (TiN+TiAlN) for machining of superalloy Inconel 718 in the dry and wet conditions was studied. The multi layer TiN and TiAlN with nanocrystalline structure was applied by physical vapor deposition technique (arc evaporation) on the WC-Co inserts. The results of the ball on disc wear test and the machinin...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Materials Research
سال: 2021
ISSN: ['0884-1616', '1092-8928', '0884-2914', '1091-8876', '2044-5326']
DOI: https://doi.org/10.1557/s43578-021-00352-w