Dislocation networks in gamma/gamma’-microstructures formed during selective laser melting of a Ni-base superalloy

نویسندگان

چکیده

A dislocation network which formed during selective laser melting (SLM) of a Ni-base superalloy was analyzed using scanning transmission electron microscopy (STEM). This traverses an ordered Gamma'-phase domain, in between two adjacent Gamma-solid solution regions. The Gamma’-phase region has when particles have started to coalesce, trapping the this so that it families with pairs anti-phase boundary (APB) coupled super partial dislocations. features are presented and unusual (twist character low APB energies), not previously reported, discussed.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

A synchrotron study of microstructure gradient in laser additively formed epitaxial Ni-based superalloy

Laser additive forming is considered to be one of the promising techniques to repair single crystal Ni-based superalloy parts to extend their life and reduce the cost. Preservation of the single crystalline nature and prevention of thermal mechanical failure are two of the most essential issues for the application of this technique. Here we employ synchrotron X-ray microdiffraction to evaluate ...

متن کامل

Thermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy

A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...

متن کامل

Carbides Evolution in a Ni-16Mo-7Cr Base Superalloy during Long-Term Thermal Exposure

The effect of long-term thermal exposure on the carbide evolution in a Ni-16Mo-7Cr base superalloy was investigated. The results show that M12C carbides are mainly precipitated on the grain boundaries during thermal exposure, and the primary massive M₆C carbides can be completely transformed to M12C carbides in situ at temperatures above 750 °C for long-term thermal exposure. The transformation...

متن کامل

Creep Crack Growth Simulation of Ni-base Superalloy

The purpose of this study is to develop a numerical approach to simulate the creep cracking of a Ni-base superalloy. The approach is based in continuum damage mechanics (CDM) and uses the classic Kachanov-Rabotnov constitutive equations for creep deformation and damage evolution. Creep damage takes the form of defects such as microcracks, cavities, voids, etc. A numerical crack growth algorithm...

متن کامل

Formation Mechanism of Silicon Modified Aluminide Coating on a Ni-Base Superalloy

Formation mechanism of silicon modified aluminide coating applied on a nickel base super alloy IN-738 LC by pack cementation process was the subject of investigation in this research. Study of the microstructure and compositions of the coating was carried out, using optical and scanning electron microscopes, EDS and X-ray diffraction (XRD) techniques. The results showed that due to low partial ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Scripta Materialia

سال: 2021

ISSN: ['1359-6462', '1872-8456']

DOI: https://doi.org/10.1016/j.scriptamat.2020.08.019