Direct Reduction of Zinc Sulfide Concentrate with Coal and Calcium Oxide
نویسندگان
چکیده
منابع مشابه
DIRECT REDUCTION OF SARCHESHME COPPER SULFIDE CONCENTRATE WITH CARBON IN THE PRESENCE OF LIME
Abstract: The direct reduction of copper sulfide concentrate from Iranian Sarcheshme deposits with carbon in the presence of lime was investigated in the temperature range of 800-1000 ºC. The reduction kinetics was determined by means of weight loss measurements. It was found that the rate of reaction increased considerably with increasing the temperature. The kinetics was also improved whe...
متن کاملSynthesis of calcium carbide-derived carbon by mechanochemical reaction of calcium carbide with sulfur, iron sulfide and zinc oxide
In the present work, we report a novel design and preparation for the mechanochemical synthesis of calcium carbide-derived carbon (CaC2-CDC) at ambient temperature. Thermodynamic calculations confirmed the possibility of calcium carbide-derived carbon formation by the reaction of calcium carbide with sulfur, iron sulfide and zinc oxide at ambient temperature. The CDCs were synthesized by the ba...
متن کاملThe Layered Reduction of Hematite (Iron Oxide) Ore by Non-Coking Coal: The Effect of Calcium Carbonate on Reduction
Due to the abundance of the non-coking coal and limitations as well as the high costs of the natural gas, the present study examined the direct reduction of hematite (iron oxide) ore in the temperature range of 800-1000 °C by the non-coking coal volatiles. Approximately, 74.9% of the total amounts of volatiles and gases exit the coal up to 800°C. The onset temperature to exit volatiles from the...
متن کاملthe layered reduction of hematite (iron oxide) ore by non-coking coal: the effect of calcium carbonate on reduction
due to the abundance of the non-coking coal and limitations as well as the high costs of the natural gas, the presentstudy examined the direct reduction of hematite (iron oxide) ore in the temperature range of 800-1000 °c by thenon-coking coal volatiles. approximately, 74.9% of the total amounts of volatiles and gases exit the coal up to800°c. the onset temperature to exit volatiles from the no...
متن کاملThe Reduction of Zinc Titanate and Zinc Oxide Solids
The reduction of bulk mixed oxides of zinc and titanium of various compositions and Zn-Ti-0 crystalline phases was studied in a thermogravimetric apparatus in Hz-H,O-N, gas mixtures at 550-1050°C. Comparative reduction experiments with ZnO were also performed. In the absence of water vapor, activation energies of 24 and 37 kcal mol’ were obtained for ZnO and Zn-Ti-0. resnectivelv. The addition ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Mining and Metallurgical Institute of Japan
سال: 1988
ISSN: 0369-4194,2185-6729
DOI: 10.2473/shigentosozai1953.104.1205_469