Development of Grain Growth Promotion Technique of Ni-Based Superalloy IN713 Fabricated by Metal Injection Molding

نویسندگان

چکیده

High temperature strength is one of the critical technical issues to apply metal injection molding (MIM) Nickel-based superalloy IN713. In this study, through investigating microstructure and high IN713-MIM materials in detail, we developed technique promote grain growth. experiments using IN713C-MIM materials, tensile creep were remarkably inferior castings. The deformation mechanism revealed that boundary diffusion was dominant as stress exponent determined n = 2.72. Therefore, found out it important reduce amount by promoting examinations aiming carbides on boundary, which inhibited migration, carbon content IN713LC-MIM-sintered material could be suppressed C 0.05%. Subsequently, when IN713LC-MIM-HIP-ed subjected additional heat treatment at 1280°C for 12 hr, significant growth observed.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Microstructure and mechanical properties of titanium components fabricated by a new powder injection molding technique

A powder injection molding (PIM) binder system has been developed for reactive metals such as titanium that employs an aromatic compound as the primary component to facilitate easy binder removal and mitigate problems with carbon contamination. In the study presented here, we examined the densification behavior, microstructure, and mechanical properties of titanium specimens formed by this proc...

متن کامل

Development and Characterization of a Metal Injection Molding Bio Sourced Inconel 718 Feedstock Based on Polyhydroxyalkanoates

The binder plays the most important role in the metal injection molding (MIM) process. It provides fluidity of the feedstock mixture and adhesion of the powder to keep the molded shape during injection molding. The binder must provide strength and cohesion for the molded part and must be easy to remove from the molded part. Moreover, it must be recyclable, environmentally friendly and economica...

متن کامل

Comparison of Interfacial Surface Tension and Capillarity of Maxillary Complete Dentures, Fabricated by Conventional Cuvette Technique and Injection Molding Technology

http://www.journal-imab-bg.org / J of IMAB. 2016, vol. 22, issue 3/ ABSTRACT Purpose: The purpose of this in vivo study is to register the forces necessary to displace maxillary complete dentures fabricated by compression molding and injection molding techniques on one and the same patient and to compare the interfacial surface tension and capillarity which are achieved by both techniques. Mate...

متن کامل

Progress in Titanium Metal Powder Injection Molding

Metal powder injection molding is a shaping technology that has achieved solid scientific underpinnings. It is from this science base that recent progress has occurred in titanium powder injection molding. Much of the progress awaited development of the required particles with specific characteristics of particle size, particle shape, and purity. The production of titanium components by injecti...

متن کامل

Development of Metal Plate with Internal Structure Utilizing the Metal Injection Molding (MIM) Process

In this study, we focus on making a double-sided metal plate with an internal structure, such as honeycomb. The stainless steel powder was used in the metal injection molding (MIM) process. The preliminary studies were carried out for the measurement of the viscosity of the stainless steel feedstock and for the prediction of the filling behavior through Computer Aided Engineering (CAE) simulati...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials transactions

سال: 2021

ISSN: ['1345-9678', '1347-5320']

DOI: https://doi.org/10.2320/matertrans.y-m2020871