Creep properties of single crystal Ni-base superalloys (SX): A comparison between conventionally cast and additive manufactured CMSX-4 materials

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys

Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys R.R. Unocic a,∗, G.B. Viswanathan a, P.M. Sarosi a, S. Karthikeyan b, J. Li a, M.J. Mills a a Department of Materials Science and Engineering, The Ohio State University, 477 Watts Hall, 2041 College Road, Columbus, OH 43210, USA b Department of Materials Engineering, Indian Institute of Science Bangalore, Karnataka 5600...

متن کامل

Temperature and Orientation Dependence of Creep Damage of Two Ni-base Superalloys

Both polycrystalline (PC) and directionally-solidified (DS) Ni-base superalloys are commonly applied as turbine materials to primarily withstand creep conditions manifested in either marine-, airor land-based gas turbines components. The thrust for increased efficiency of these systems, however, translates into the need for these materials to exhibit considerable strength and temperature resist...

متن کامل

High Temperature Nanoindentation of Ni-base Superalloys

Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...

متن کامل

CONSTITUTIVE MODELING OF CREEP OF SINGLE CRYSTAL SUPERALLOYS A Dissertation by SHARAT CHAND PRASAD

Constitutive Modeling of Creep of Single Crystal Superalloys. (August 2005) Sharat Chand Prasad, B.Tech., Indian Institute of Technology, Kanpur; M.S., Texas A&M University Chair of Advisory Committee: Dr. K. R. Rajagopal In this work, a constitutive theory is developed, within the context of continuum mechanics, to describe the creep deformation of single crystal superalloys. The constitutive ...

متن کامل

Effects of Alloying Elements on Elastic, Stacking Fault, and Diffusion Properties of Fcc Ni from First-principles: Implications for Tailoring the Creep Rate of Ni-base Superalloys

To understand the effects of alloying elements on the creep rate of Ni-base superalloys, factors entering into a secondary creep rate are calculated via first-principles calculations based on density functional theory for 26 Ni31X systems where X = Al, Co, Cr, Cu, Fe, Hf, Ir, Mn, Mo, Nb, Os, Pd, Pt, Re, Rh, Ru, Sc, Si, Ta, Tc, Ti, V, W, Y, Zr, and Zn. They are volume, elastic properties, stacki...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials Science and Engineering: A

سال: 2019

ISSN: 0921-5093

DOI: 10.1016/j.msea.2019.138098