Creep properties of different γ′-strengthened Co-base superalloys
نویسندگان
چکیده
منابع مشابه
Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys
Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys R.R. Unocic a,∗, G.B. Viswanathan a, P.M. Sarosi a, S. Karthikeyan b, J. Li a, M.J. Mills a a Department of Materials Science and Engineering, The Ohio State University, 477 Watts Hall, 2041 College Road, Columbus, OH 43210, USA b Department of Materials Engineering, Indian Institute of Science Bangalore, Karnataka 5600...
متن کاملModelling the creep anisotropy of nickel-base superalloys with a composite model
The creep anisotropy of nickel-base superalloys with a cubic y' morphology is studied with a composite model. Creep curves and the internal stress distribution in the microstructure under [Oll] load are calculated with a Finite Element Procedure. Analytical considerations are made for arbitrary loading directions. y' cubes (with their interfaces aligned parallel to (001) planes) under [OOl] loa...
متن کاملTemperature and Orientation Dependence of Creep Damage of Two Ni-base Superalloys
Both polycrystalline (PC) and directionally-solidified (DS) Ni-base superalloys are commonly applied as turbine materials to primarily withstand creep conditions manifested in either marine-, airor land-based gas turbines components. The thrust for increased efficiency of these systems, however, translates into the need for these materials to exhibit considerable strength and temperature resist...
متن کاملOpen-Cellular Co-Base and Ni-Base Superalloys Fabricated by Electron Beam Melting
Reticulated mesh samples of Co-29Cr-6Mo alloy and Ni-21Cr-9Mo-4Nb alloy (625) and stochastic foam samples of Co-29Cr-6Mo alloy fabricated by electron beam melting were characterized by optical metallography, and the dynamic stiffness (Young's modulus) was measured by resonant frequency analysis. The relative stiffness (E/Es) versus relative density (ρ/ρs) plotted on a log-log basis resulted in ...
متن کاملinvestigation of gassing behavior, electric and dielectric properties of different insulating fluids.
ترانسفورماتورهای قدرت از اجزای اصلی شبکه تامین انرژی الکتریکی می باشند که عملکرد قابل اطمینان ترانسفورماتورها یکی از فاکتورهای مهم و تعیین کننده در تامین انرژی الکتریکی محسوب می شود. در نتیجه بررسی و مانیتور عملکرد ترانسفورماتورها در شبکه و همچنین عیب یابی این ترانسفورماتورها غیرقابل اجتناب و ضروری می باشد. به طور کلی عایق های مایع در صنعت فشار قوی کاربردهای متفاوتی دارند که مهمترین وظیفه آنها...
15 صفحه اولذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Materials Science and Engineering: A
سال: 2012
ISSN: 0921-5093
DOI: 10.1016/j.msea.2012.04.083