Creep-Induced Microstructural Changes in Large Welded Joints of High Cr Heat Resistant Steel

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Creep Deformation Measurement of 316H Stainless Steel Multi-pass Welded Joints using Digital Image Correlation

A high temperature measurement system for creep deformation based on the digital image correlation (DIC) technique is described. The new system is applied to study the behaviour of a multi-pass welded joint in a high temperature tensile test and a load controlled creep test at 545°C. Spatially resolved tensile properties and time dependent creep deformation properties across a thick section typ...

متن کامل

Microstructural Properties of Semisolid Welded Joints for AISI D 2 Tool Steel

The aim of this study is to investigate experimentally the microstructural evolution of the joints using ledeburitic AISI D2 Tool Steel parts. The application of a new process of the semisolid joining of two parts of AISI D2 cold-work tool steel is proposed using a partial remelting method. Samples were heated in an argon atmosphere up to 1300°C and held for 10 minutes. Metallographic analyses ...

متن کامل

Microstructural Investigation of the Heat-affected Zone of Simulated Welded Joint of P91 Steel

T. Vuherer, University of Maribor, Faculty of Mechanical Engineering, Slovenia, M. Dunđer, University of Rijeka, Politechnika Department of Philosophy Faculty, Croatia, I. Samardžić, University of Osijek, Mechanical Engineering Faculty, Slav. Brod, Croatia, Lj. Milović, University of Belgrade, Faculty of Technology and Metallurgy, Serbia, M. Zrilić, University of Belgrade, Faculty of Technology...

متن کامل

Creep behavior and in-depth microstructural characterization of dissimilar joints

The 700 °C power plants currently under development will utilize Ni-base alloys such as alloy 617 for components to be operated at temperatures >650 °C. Due to economic reasons for components or parts of components which are subjected to temperatures <650 °C, 2% Cr or 9-12% Cr steels is used, depending on the required mechanical properties. This makes the dissimilar joining of Ni-base alloys an...

متن کامل

The Influence of Ultrasonic Impact Treatment on Fatigue Behaviour of Welded Joints in High-strength Steel

The unabated growth of the steel industry and progressively increasing operating loads on metal structures generate a need for a search for optimum engineering solutions to improve the loadcarrying capacity and reduce metal consumption. One way of resolving this problem is to utilise high-strength steels. It is common knowledge however that the improvement of the steel strength is accompanied b...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Procedia Engineering

سال: 2013

ISSN: 1877-7058

DOI: 10.1016/j.proeng.2013.03.216