Creep Failure Process for Fine Powder Beds by Tensile Loading.
نویسندگان
چکیده
منابع مشابه
A nano-tensile tester for creep studies
Free-standing metallic thin films are increasingly used as structural components in MEMS. In commercial devices, long-term reliability is essential, which requires determining time-dependent mechanical properties of these films. The uniaxial tensile test is a preferred method due to uncomplicated determination of the stress and strain state. However, at the MEMS-scale this method is not straigh...
متن کاملFailure of Aβ(1-40) amyloid fibrils under tensile loading.
Amyloid fibrils and plaques are detected in the brain tissue of patients affected by Alzheimer's disease, but have also been found as part of normal physiological processes such as bacterial adhesion. Due to their highly organized structures, amyloid proteins have also been used for the development of nanomaterials, for a variety of applications including biomaterials for tissue engineering, na...
متن کاملFailure of Ab(1-40) amyloid fibrils under tensile loading
Amyloid fibrils and plaques are detected in the brain tissue of patients affected by Alzheimer’s disease, but have also been found as part of normal physiological processes such as bacterial adhesion. Due to their highly organized structures, amyloid proteins have also been used for the development of nanomaterials, for a variety of applications including biomaterials for tissue engineering, na...
متن کاملTensile creep behaviour of polymethylpentenesilica nanocomposites
For the first time, poly(4-methyl-1-pentene) (PMP) nanocomposites were prepared by melt compounding 2 vol% of fumed silica nanoparticles, in order to study the role of the nanofiller surface area and functionalization on the tensile mechanical response of the material, with particular focus on its creep behaviour. The high optical transparency of the polymer matrix was substantially preserved i...
متن کاملTensile Creep of Polycrystalline Near-Stoichiometric NiAl
Long term tensile creep studies were conducted on binary NiAl in the temperature range 700-1200 K with the objectives of characterizing and understanding the creep mechanisms. Inverse and normal primary creep curves were observed depending on stress and temperature. It is concluded that the primary creep of NiAl is limited by dislocation mobility. The stress exponent for creep, n, decreased fro...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: KAGAKU KOGAKU RONBUNSHU
سال: 1994
ISSN: 0386-216X,1349-9203