Cover Feature: 2D FeS<sub><i>x</i></sub> Nanosheets by Atomic Layer Deposition: Electrocatalytic Properties for the Hydrogen Evolution Reaction (ChemSusChem 11/2023)

نویسندگان

چکیده

The Cover Feature shows a scheme of the synthesis by atomic layer deposition 2D iron sulfide nanosheets conformal and homogenously grown on titanium dioxide nanotube layers. Those composite nanotubular structures feature electrocatalytic activity toward hydrogen evolution reaction in alkaline media, originated from synergistic interplay between situ both morphological chemical composition changes experienced nanosheets. More information can be found Research Article R. Zazpe et al.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Preparation of Ni-P-CeO2 electrode and study on electrocatalytic properties for hydrogen evolution reaction

In this study ternary Ni-P-CeO2 catalysts were first synthesized by the Co-electrodeposition method on a copper substrate and then characterized by means of microstructural and electrochemical techniques toward a hydrogen evolution reaction (HER). Also, for comparison other catalysts such as Ni-CeO2, Ni-P, and Ni were prepared and characterized by the same methods. The microstructure of the inv...

متن کامل

Porous metallic MoO2-supported MoS2 nanosheets for enhanced electrocatalytic activity in the hydrogen evolution reaction.

Advanced materials for electrocatalytic water splitting are central to renewable energy research. In this work, MoS2 nanosheets supported on porous metallic MoO2 (MoS2/MoO2) were produced by sulfuration treatments of porous and highly conductive MoO2 for the hydrogen evolution reaction. Porous MoO2 with one-dimensional channel-like structures was prepared by calcination at elevated temperatures...

متن کامل

Recent Strategies for Improving the Catalytic Activity of 2D TMD Nanosheets Toward the Hydrogen Evolution Reaction.

Two-dimensional (2D) transition-metal dichalcogenide (TMD) nanosheets have emerged as a fascinating new class of materials for catalysis. These nanosheets are active for several important catalysis reactions including hydrogen evolution from water. The rich chemistry of TMDs combined with numerous strategies that allow tuning of their electronic properties make these materials very attractive f...

متن کامل

High turnover frequency of hydrogen evolution reaction on amorphous MoS2 thin film directly grown by atomic layer deposition.

Recently amorphous MoS2 thin film has attracted great attention as an emerging material for electrochemical hydrogen evolution reaction (HER) catalyst. Here we prepare the amorphous MoS2 catalyst on Au by atomic layer deposition (ALD) using molybdenum hexacarbonyl (Mo(CO)6) and dimethyl disulfide (CH3S2CH3) as Mo and S precursors, respectively. Each active site of the amorphous MoS2 film effect...

متن کامل

Hierarchical spheres constructed by defect-rich MoS2/carbon nanosheets for efficient electrocatalytic hydrogen evolution

Highly active and stable MoS2/carbon hierarchical spheres with abundant active edge sites were fabricated by a simple micro-emulsion procedure where PVP was used as the carbon source, and carbon disulfide as the sulfur source and oil phase in micro-emulsion to control the morphology of MoS2. Hierarchical spheres of MoS2/carbon with a diameter of ca. 500 nm were obtained and characterized by sca...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Chemsuschem

سال: 2023

ISSN: ['1864-5631', '1864-564X']

DOI: https://doi.org/10.1002/cssc.202300668