Corrosion Behavior of AISI 304 Stainless Steel in Aggressive Chloride Environment

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Enhancement of corrosion protection of AISI 304 stainless steel by nanostructured sol–gel TiO2 films

0010-938X/$ see front matter 2013 Elsevier Ltd. All rights reserved. http://dx.doi.org/10.1016/j.corsci.2013.07.045 ⇑ Corresponding author. Address: Faculty of Mechanical Engineering and Naval Architecture, Departmet of Materials, Ivana Lučića 5, 10000 Zagreb, Croatia. Tel.: +385 1 616 8313; fax: +385 1 615 7126. E-mail address: [email protected] (L. Ćurković). Lidija Ćurković a,⇑, Helena ...

متن کامل

Micro abrasion-corrosion of AISI 316L stainless steel

In this study, the synergistic effects of abrasion and corrosion on AISI 316L stainless steel have been investigated using a micro-abrasion test rig. A series of results from abrasioncorrosion tests conducted using the micro-abrasion rig are presented. AISI 316L stainless steel has been studied under both pure abrasion and abrasion-corrosion conditions simulated by either distilled water or 3.5...

متن کامل

Passivation and corrosion behaviours of AISI 316L stainless steel as implant materials in simulated blood environment

The purpose of the study was evaluation of corrosion resistance of steel 316L used in cardiologic treatment mainly for vascular stents. The study analysed influence of electrochemical and chemical treatment of the steel surface, including sterilisation with pressurised water steam, on its corrosion characteristics. The tests were performed in artificial blood plasma simulating human blood envir...

متن کامل

Corrosion Behavior of Stainless Steel Clad Rebar

Stainless steel clad rebar (SCR) was investigated because it may become a cost-effective means of controlling corrosion in concrete under very aggressive environments. Sound SCR (316L cladding) resisted corrosion in saturated Ca(OH)2 solution (SCS) with up to 5 wt% chloride. Cladding breaks on SCR induced significant corrosion of exposed underlying CS in SCS with only 1 wt% chloride. A computer...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Manufacturing Technology

سال: 2017

ISSN: 1213-2489,1213-2489

DOI: 10.21062/ujep/x.2017/a/1213-2489/mt/17/4/639