Characterization and Investigation of Grain Selection in Spiral Grain Selectors during Casting Single-Crystal Turbine Blades

Manufactured single crystal components using Ni-base super alloys are routinely used in the hot sections of aero engines and industrial gas turbines due to their outstanding high temperature strength, toughness and resistance to degradation in corrosive and oxidative environments. To control the quality of the single crystal turbine blades, particular attention has been paid to grain selection,...

متن کامل

Characterization and Investigation of Grain Selection in Spiral Grain Selectors during Casting Single-Crystal Turbine Blades

Manufactured single crystal components using Ni-base super alloys are routinely used in the hot sections of aero engines and industrial gas turbines due to their outstanding high temperature strength, toughness and resistance to degradation in corrosive and oxidative environments. To control the quality of the single crystal turbine blades, particular attention has been paid to grain selection,...

متن کامل

characterization and investigation of grain selection in spiral grain selectors during casting single-crystal turbine blades

manufactured single crystal components using ni-base super alloys are routinely used in the hotsections of aero engines and industrial gas turbines due to their outstanding high temperaturestrength, toughness and resistance to degradation in corrosive and oxidative environments. tocontrol the quality of the single crystal turbine blades, particular attention has been paid to grainselection, whi...

متن کامل

On APFIM of Grain Boundaries in a Nickel Base Superalloy

Experimental details of atom probe field ion microscopy (APFIM) of a Ni-16Cr-9Fe alloy are presented. In particular, studies concerning analysis of intergranular carbides and borides and segregation to grain boundaries are described. It was found that NiZ3B6 precipitates are very sensitive to preferential field evaporation, which necessitates optimization of the analysis conditions. In the FIM ...

متن کامل

Joining of nickel-base superalloy single crystals

Introduction ................................................................................................................................1 Overview of Weldability of Nickel-Base Superalloys..................................................................1 Crystallography............................................................................................................................

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Crystals

سال: 2022

ISSN: ['2073-4352']

DOI: https://doi.org/10.3390/cryst12101384