Copper extraction from copper smelter slag with pyrite or flotation tailings followed by water leaching
نویسندگان
چکیده
منابع مشابه
Recovery of Copper from Copper Slag and Copper Slag Flotation Tailings by Oxidative Leaching
Copper smelter slag and copper smelter slag flotation tailings were leached using sulphuric acid solutions, without or with the addition of either ferric sulphate or hydrogen peroxide. Copper extraction from the slag was typically found to be twice as high as that from the slag flotation tailings. Hydrogen peroxide was determined to be the best lixiviant. Thus, copper and iron extractions were ...
متن کاملSolvent extraction of Cu, Mo, V, and U from leach solutions of copper ore and flotation tailings
Flotation tailings from copper production are deposits of copper and other valuable metals, such as Mo, V and U. New hydrometallurgical technologies are more economical and open up new possibilities for metal recovery. This work presents results of the study on the extraction of copper by mixed extractant consisting p-toluidine dissolved in toluene. The possibility of simultaneous liquid-liquid...
متن کاملExtraction of Tin and Copper by Acid Leaching of PCBs
Printed circuit board (PCB) waste is generally dumped as a landfilling or treated pyrometallurg ically, which consumes enormous power, generates hazardous gases and also destroys valuable PCB components. For recycling of the components, they must be separated from the printed circuit boards which is a cumbersome task. For its simplification, the rate of d issolution of solder with acids like Hy...
متن کاملMortality from Copper Smelter Emissions Circa 1967
Pope et al. (2007) found lowered monthly mortality rates during a 1967–1968 copper smelter strike, coincident with and attributed to widespread reduced airborne sulfate levels. The authors cited three “intervention” studies associating particulate emissions reductions with mortality reductions as supportive. Evidence below suggests that mortality reductions in the study by Pope et al. and “inte...
متن کاملExtraction of Lithium from Lepidolite Using Mixed Grinding with Sodium Sulfide Followed by Water Leaching
Mixed grinding with Na2S followed by water leaching was performed to extract Li from lepidolite. The leachability of Li increases dramatically in the ground mixture, regardless of the mixing ratio over the range of 1:1 to 3:1, while only 4.53% of Li was extracted in lepidolite ground without Na2S. The leachability increased with an increase of the grinding time, and ultimately, 93% of the Li wa...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Mining and Metallurgy Engineering Bor
سال: 2014
ISSN: 2334-8836
DOI: 10.5937/mmeb1404157d