Characterization of the Weld Line Zones of an Inertia Friction Welded Superalloy
نویسندگان
چکیده
منابع مشابه
determination of maximal singularity free zones in the workspace of parallel manipulator
due to the limiting workspace of parallel manipulator and regarding to finding the trajectory planning of singularity free at workspace is difficult, so finding a best solution that can develop a technique to determine the singularity-free zones in the workspace of parallel manipulators is highly important. in this thesis a simple and new technique are presented to determine the maximal singula...
15 صفحه اولinfluence of weld process parameters on material characterization of friction stir welded joints of aluminium alloy aa6061-t6
abstract: friction stir welding, a solid state innovative joining technique, is widely being used for joining aluminium alloys for aerospace, marine automotive and many other applications of commercial importance. fsw trials were carried out using a vertical machining centre (vmc) on aa6061 alloy. the main objective of the present work was to evaluate the weld processing parameter of friction s...
متن کاملStudy the Profile Shape and Mechanical Properties of Bonded Joint HNV3 to Nimonic 80A Superalloy with Inertia Friction Welding Method
This Paper presents the welding parameterchr('39')s effect (forging pressure, welding time) on macrostructure and mechanical properties of friction welding valve steel HNV3 to Nimonic 80A super alloy. For this purpose, two rods with 20 mm diameters are prepared and with using different parameters (Increase forging pressure and welding time) by friction welding method are welded together. Tensil...
متن کاملStudy the Profile Shape and Mechanical Properties of Bonded Joint HNV3 to Nimonic 80A Superalloy with Inertia Friction Welding Method
This Paper presents the welding parameterchr('39')s effect (forging pressure, welding time) on macrostructure and mechanical properties of friction welding valve steel HNV3 to Nimonic 80A super alloy. For this purpose, two rods with 20 mm diameters are prepared and with using different parameters (Increase forging pressure and welding time) by friction welding method are welded together. Tensil...
متن کاملInfluence of Weld Process Parameters on Material Characterization of Friction Stir Welded Joints of Aluminium Alloy AA6061-T6
Friction stir welding, a solid state innovative joining technique, is widely being used to join aluminium alloys for aerospace, marine automotive and many other applications of commercial importance. FSW trials were carried out using a vertical machining centre (VMC) on AA6061 alloy. The main objective of the present work was to evaluate the weld processing parameter of friction stir weld (FSW)...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Advanced Materials Research
سال: 2011
ISSN: 1662-8985