CHARACTERIZATION OF HYDROTHERMALLY SYNTHESISED HYDROXYAPATITE BIOCERAMIC
نویسندگان
چکیده
منابع مشابه
Synthesis and Characterization of Carbonated Hydroxyapatite as Bioceramic Material Widyastuti
xv CHAPTER I: INTRODUCTION 1.1 Background and Problem Statement 1 1.2 Objectives of the Research 4 1.3 Project Overview 5 CHAPTER II: LITERATURE REVIEW 2.
متن کاملHydrothermally processed 1D hydroxyapatite: Mechanism of formation and biocompatibility studies.
Recent developments in bone tissue engineering have led to an increased interest in one-dimensional (1D) hydroxyapatite (HA) nano- and micro-structures such as wires, ribbons and tubes. They have been proposed for use as cell substrates, reinforcing phases in composites and carriers for biologically active substances. Here we demonstrate the synthesis of 1D HA structures using an optimized, ure...
متن کاملFabrication of Macrochannelled-Hydroxyapatite Bioceramic by a Coextrusion Process
A coextrusion process was used to fabricate macrochannelled hydroxyapatite (HA). To improve the powder characteristics, the HA powder was calcined at 900°C in air for 1 h. A feedrod composed of HA (shell) and carbon black (core) was coextruded at 120°C through a symmetric 8:1 square reduction die. After the first coextrusion, the individual pieces were bundled, warm-pressed, and then coextruded...
متن کاملCrystallographic texture in pulsed laser deposited hydroxyapatite bioceramic coatings.
The orientation texture of pulsed laser deposited hydroxyapatite coatings was studied by X-ray diffraction techniques. Increasing the laser energy density of the KrF excimer laser used in the deposition process from 5 to 7 J/cm(2) increases the tendency for the c-axes of the hydroxyapatite grains to be aligned perpendicular to the substrate. This preferred orientation is most pronounced when th...
متن کاملHydroxyapatite - starch nano biocomposites synthesis and characterization
Bone like hydroxyapatite (nHAp) was synthesized via an in situ biomimetic process in presence of wheat starch. The effect of polymer concentration alteration on the final structure of nHAp was investigated. Formation of the nHAp at room temperature was confirmed by X-ray diffraction (XRD) and Fourier transform infrared spectroscopy (FT-IR). Size and morphology of the nHAp samples were character...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Turkish Journal of Engineering
سال: 2018
ISSN: 2587-1366
DOI: 10.31127/tuje.327822