Chairside Fabrication of an All-Ceramic Partial Crown Using a Zirconia-Reinforced Lithium Silicate Ceramic

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Chairside Fabrication of an All-Ceramic Partial Crown Using a Zirconia-Reinforced Lithium Silicate Ceramic

The chairside fabrication of a monolithic partial crown using a zirconia-reinforced lithium silicate (ZLS) ceramic is described. The fully digitized model-free workflow in a dental practice is possible due to the use of a powder-free intraoral scanner and the computer-aided design/computer-assisted manufacturing (CAD/CAM) of the restorations. The innovative ZLS material offers a singular combin...

متن کامل

Fabrication of Zirconia-Reinforced Lithium Silicate Ceramic Restorations Using a Complete Digital Workflow

This case report describes the fabrication of monolithic all-ceramic restorations using zirconia-reinforced lithium silicate (ZLS) ceramics. The use of powder-free intraoral scanner, generative fabrication technology of the working model, and CAD/CAM of the restorations in the dental laboratory allows a completely digitized workflow. The newly introduced ZLS ceramics offer a unique combination ...

متن کامل

Somaraj V: Esthetic Rehabilitation using Zirconia-Based All-Ceramic Crown

The dental practice is not only about prevention and treatment of oral diseases but also the fulfillment of demands of all who seek oral care, of which esthetics weighs more importance than any. To achieve excellence in the delivery of dental care, dentists rely on the vast array of modern advances in dental materials and restoration fabrication technologies. Need for more esthetical, metal-fre...

متن کامل

Effect of Lithium Disilicate Reinforced Liner Treatment on Bond and Fracture Strengths of Bilayered Zirconia All-Ceramic Crown

This study was performed to evaluate the effect of a lithium-disilicate spray-liner application on both the bond strength between zirconia cores and heat-pressed lithium-disilicate glass-ceramic veneers, and the fracture strength of all-ceramic zirconia crowns. A lithium-disilicate reinforced liner was applied on the surface of a zirconia core and lithium-disilicate glass-ceramic was veneered o...

متن کامل

Thermal shock resistance of core reinforced all-ceramic crown systems.

The coefficient of thermal expansion of core and veneer porcelains for all ceramic crowns must be compatible to prevent formation of stresses during the firing cycles. The purpose of this study was to use a thermal shock test to evaluate the crazing resistance of six all-ceramic crown systems. The systems tested were: Vita In-Ceram, Vita Hi-Ceram, Dicor veneered with Vitadur N, magnesia core ve...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Case Reports in Dentistry

سال: 2016

ISSN: 2090-6447,2090-6455

DOI: 10.1155/2016/1354186