Atomic layer deposition of Nb-doped ZnO for thin film transistors

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Bi-layer Channel AZO/ZnO Thin Film Transistors Fabricated by Atomic Layer Deposition Technique

This letter demonstrates bi-layer channel Al-doped ZnO/ZnO thin film transistors (AZO/ZnO TFTs) via atomic layer deposition process at a relatively low temperature. The effects of annealing in oxygen atmosphere at different temperatures have also been investigated. The ALD bi-layer channel AZO/ZnO TFTs annealed in dry O2 at 300 °C exhibit a low leakage current of 2.5 × 10-13A, I on/I off ratio ...

متن کامل

Al-Doped ZnO Thin Film Transistors by Thermal Evaporation

In this paper, Al-doped ZnO thin film transistors (AZO-TFT) were fabricated by the thermal evaporation growth of AZO channel layer on a silicon substrate at temperatures below 250°C. A SiO2 dielectric layer grown by the horizontal furnace was used as a gate. An active layer thickness of 10nm was measured by Atomic Force Microscopy (AFM), and its surface had root mean square (rms) roughness 12.6...

متن کامل

Atomic-Layer-Deposition of Indium Oxide Nano-films for Thin-Film Transistors

Atomic-layer-deposition (ALD) of In2O3 nano-films has been investigated using cyclopentadienyl indium (InCp) and hydrogen peroxide (H2O2) as precursors. The In2O3 films can be deposited preferentially at relatively low temperatures of 160-200 °C, exhibiting a stable growth rate of 1.4-1.5 Å/cycle. The surface roughness of the deposited film increases gradually with deposition temperature, which...

متن کامل

Process Optimization of Deposition Conditions for Low Temperature Thin Film Insulators used in Thin Film Transistors Displays

Deposition process for thin insulator used in polysilicon gate dielectric of thin film transistors are optimized. Silane and N2O plasma are used to form SiO2 layers at temperatures below 150 ºC. The deposition conditions as well as system operating parameters such as pressure, temperature, gas flow ratios, total flow rate and plasma power are also studied and their effects are discussed.  The p...

متن کامل

Atomic layer deposition (ALD): from precursors to thin film structures

The principles of the atomic layer deposition (ALD) method are presented emphasizing the importance of precursor and surface chemistry. With a proper adjustment of the experimental conditions, i.e. temperatures and pulsing times, the growth proceeds via saturative steps. Selected recent ALD processes developed for films used in microelectronics are described as examples. These include depositio...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Applied Physics Letters

سال: 2016

ISSN: 0003-6951,1077-3118

DOI: 10.1063/1.4968194