Applications of atomic layer deposition in solar cells.
Atomic layer deposition (ALD) provides a unique tool for the growth of thin films with excellent conformity and thickness control down to atomic levels. The application of ALD in energy research has received increasing attention in recent years. In this review, the versatility of ALD in solar cells will be discussed. This is specifically focused on the fabrication of nanostructured photoelectro...
متن کاملMaking Record-efficiency SnS Solar Cells by Thermal Evaporation and Atomic Layer Deposition.
Tin sulfide (SnS) is a candidate absorber material for Earth-abundant, non-toxic solar cells. SnS offers easy phase control and rapid growth by congruent thermal evaporation, and it absorbs visible light strongly. However, for a long time the record power conversion efficiency of SnS solar cells remained below 2%. Recently we demonstrated new certified record efficiencies of 4.36% using SnS dep...
متن کاملIntermittent Very High Frequency Plasma Deposition on Microcrystalline Silicon Solar Cells Enabling High Conversion Efficiency
Stopping the plasma-enhanced chemical vapor deposition (PECVD) once and maintaining the film in a vacuum for 30 s were performed. This was done several times during the formation of a film of i-layer microcrystalline silicon (μc-Si:H) used in thin-film silicon tandem solar cells. This process aimed to reduce defect regions which occur due to collision with neighboring grains as the film becomes...
متن کاملInterface Engineering through Atomic Layer Deposition towards Highly Improved Performance of Dye-Sensitized Solar Cells
A composite photoanode comprising ultralong ZnO nanobelts and TiO2 nanoparticles was prepared and its performance in dye-sensitized solar cells (DSSCs) was optimized and compared to the photoanode consisting of conventional TiO2 nanoparticles. The ultralong ZnO nanobelts were synthesized in high yield by a facile solution approach at 90°C followed by annealing at 500°C. The effect of the ratio ...
متن کاملToward plasmonic solar cells: protection of silver nanoparticles via atomic layer deposition of TiO2.
Plasmonic silver nanoparticles have unique properties that lend themselves to unusual optical applications, potentially including use as absorption amplifiers in dye-sensitized solar cells (DSSCs). However, these particles are easily damaged under oxidizing conditions. Atomic layer deposition of TiO2 onto transparent-conductive-oxide-supported silver particles was examined as a means of protect...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Nano Materials Science
سال: 2020
ISSN: 2589-9651
DOI: 10.1016/j.nanoms.2019.10.001