A Study on Solution-Processed Y2O3 Films Modified by Atomic Layer Deposition Al2O3 as Dielectrics in ZnO Thin Film Transistor

نویسندگان

چکیده

In this work, Y2O3–Al2O3 dielectrics were prepared and used in ZnO thin film transistor as gate insulators. The Y2O3 by the sol–gel method has many surface defects, resulting a high density of interface states with active layer TFT, which then leads to poor stability devices. We modified it atomic deposition (ALD) technology that deposited Al2O3 on dielectric layer, finally fabricated TFT device ALD. electrical performance bias laminated greatly improved, subthreshold swing was reduced from 147 88 mV/decade, on/off-state current ratio increased 4.24 × 106 4.16 108, threshold voltage shift 1.4 0.7 V after 5-V is applied for 800 s.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Bi-layer Channel AZO/ZnO Thin Film Transistors Fabricated by Atomic Layer Deposition Technique

This letter demonstrates bi-layer channel Al-doped ZnO/ZnO thin film transistors (AZO/ZnO TFTs) via atomic layer deposition process at a relatively low temperature. The effects of annealing in oxygen atmosphere at different temperatures have also been investigated. The ALD bi-layer channel AZO/ZnO TFTs annealed in dry O2 at 300 °C exhibit a low leakage current of 2.5 × 10-13A, I on/I off ratio ...

متن کامل

On the environmental stability of ZnO thin films by spatial atomic layer deposition

• A submitted manuscript is the author's version of the article upon submission and before peer-review. There can be important differences between the submitted version and the official published version of record. People interested in the research are advised to contact the author for the final version of the publication, or visit the DOI to the publisher's website. • The final author version ...

متن کامل

Effects of Al Doping on the Properties of ZnO Thin Films Deposited by Atomic Layer Deposition

The tuning of structural, optical, and electrical properties of Al-doped ZnO films deposited by atomic layer deposition technique is reported in this work. With the increasing Al doping level, the evolution from (002) to (100) diffraction peaks indicates the change in growth mode of ZnO films. Spectroscopic ellipsometry has been applied to study the thickness, optical constants, and band gap of...

متن کامل

Thermo-Optical Properties of Thin-Film TiO2–Al2O3 Bilayers Fabricated by Atomic Layer Deposition

We investigate the optical and thermo-optical properties of amorphous TiO2–Al2O3 thin-film bilayers fabricated by atomic layer deposition (ALD). Seven samples of TiO2–Al2O3 bilayers are fabricated by growing Al2O3 films of different thicknesses on the surface of TiO2 films of constant thickness (100 nm). Temperature-induced changes in the optical refractive indices of these thin-film bilayers a...

متن کامل

Effect of the Hydrophobicity of Hybrid Gate Dielectrics on a ZnO Thin Film Transistor

Amorphous silicon thin film transistors (a-Si TFTs) are widely used for consumer electronics and have been demonstrated to be useful for use in solar cells and flexible displays. Organic thin film transistors are of interest for applications in low-cost electronic devices such as radio-frequency identification tags, flexible displays, memory and sensors. However, the applications of these devic...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Coatings

سال: 2021

ISSN: ['2079-6412']

DOI: https://doi.org/10.3390/coatings11080969