7.6% CZGSe Solar Cells Thanks to Optimized CdS Chemical Bath Deposition

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Preparation of Nanocrystalline CdS Thin Films by a New Chemical Bath Deposition Route for Application in Solar Cells as Antireflection Coatings

Nanocrystalline cadmium sulfide thin films as antireflection materials for solar cells have been prepared by a new chemical solution deposition route in an aqueous medium at 50 °C. as-deposited thin films were studied using X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), and optical absorption spectra. X-ray diffraction data indicated the formation of hexagonal na...

متن کامل

Comparison of Close-Spaced Sublimated and Chemical Bath Deposited CdS Films: Effects on CdTe Solar Cells

Close-spaced-sublimated (CSS) CdS films exhibit strong fundamental edge luminescence, high optical absorption, and a bandgap of ~2.41 eV. Structurally, these films show good crystallinity with thickness-dependent grain sizes that vary between 100-400 nm. In contrast, chemical-bath-deposited (CBD) CdS exhibits subband luminescence, lower absorption, and a thicknessdependent bandgap. These films ...

متن کامل

Chemical Bath Deposited CdS for CdTe and Cu(In,Ga)Se2 Thin Film Solar Cells Processing

Extensive research has been done during the last two decades on cadmium sulfide (CdS) thin films, mainly due to their application to large area electronic devices such as thin film field-effect transistors (Schon et al., 2001) and solar cells (Romeo et al., 2004). For the latter case, chemical bath deposited (CBD) CdS thin films have been used extensively in the processing of CdTe and Cu(In,Ga)...

متن کامل

STRUCTURAL, OPTICAL AND ELECTRICAL PROPERTIES OF NANOCRYSTALLINE CdS THIN FILMS GROWN BY CHEMICAL BATH DEPOSITION METHOD

Cadmium sulfide thin films are prepared on glass substrates at 82 °C for 1 hour by chemical bath deposition. After deposition, the films are annealed at 480 °C for 1 hour in air atmosphere. Both as-grown and annealed films are characterized by X-ray diffraction, scanning electron microscopy, energy dispersive spectroscopy, optical absorption spectroscopy and current voltage characteristics and ...

متن کامل

A New Route for Preparing CdS thin Films by Chemical Bath Deposition Using EDTA as Ligand

Progress is reported towards the development of a new route to obtain cadmium sulfide (CdS) thin films by using ethylene-diamine-tetra-acetic acid (EDTA) ligand on the chemical bath deposition (CBD) method. Different chemical baths are used to study changes in the structures of the CdS films for different EDTA concentrations. X-ray diffraction (XRD) is used to prove the structural characterizat...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: physica status solidi (a)

سال: 2018

ISSN: 1862-6300

DOI: 10.1002/pssa.201800043