A group of Stellite alloys are studied in consideration of temperature effects on their hardness and wear resistance. The hardness test is conducted on a micro-hardness tester with a hot stage equipped that allows heating the specimen up to 650°C. The wear resistance of each alloy is evaluated using a pin-on-disc tribometer with a heating furnace built-in that provides the temperature capacity ...
The microstructure and wear resistance of Stellite 6 alloy hardfacing layer at two different temperatures (room temperature and 300°C) were investigated by plasma arc surfacing processes on Q235 Steel. Tribological test was conducted to characterize the wear property. The microstructure of Stellite 6 alloy coating mainly consists of α-Co and (Cr, Fe)7C3 phases. The friction coefficient of Stell...
OBJECTIVE To study exposure to cobalt and chromium in saw maintenance rooms and test respiratory health among saw filers at lumber mills. Hard-metal lung disease is associated with cobalt in the manufacture of tungsten carbide tools; recently it has also been reported among tool maintenance workers. Lumber mills often use saws tipped with tungsten carbide or with a newer alloy, stellite (contai...
Increased destruction of red blood cells follows the insertion of ball valves into the heart in most cases. Usually, hemolysis is slight, but in some patients uncompensated hemolytic anemia develops. To study the influence on hemolysis of the mechanical properties of the prostheses, the degree of erythrocyte destruction was evaluated in patients with Starr-Edwards aortic prostheses of different...
Increased destruction of red blood cells follows the insertion of ball valves into the heart in most cases. Usually, hemolysis is slight, but in some patients uncompensated hemolytic anemia develops. To study the influence on hemolysis of the mechanical properties of the prostheses, the degree of erythrocyte destruction was evaluated in patients with Starr-Edwards aortic prostheses of different...
K465 superalloy with high titanium and aluminum contents was easy to crack during laser metal deposition. In this study, the crack-free sample of K465/Stellite-6 laminated material was formed by laser metal deposition shaping to control the cracking behaviour in laser metal deposition of K465 superalloy. The microstructure differences between the K465 superalloy with cracking and the laminated ...
From the wide range of engineering materials traditional Stellite 6 (cobalt alloy) exhibits excellent resistance to cavitation erosion (CE). Nonetheless, influence ion implantation cobalt alloys on CE behaviour has not been completely clarified by literature. Thus, this work investigates effect nitrogen (NII) HIPed improvement CE. Finally, cobalt-rich matrix phase transformations due both NII a...
This paper deals with the investigation of the microstructure and hardness of steel samples cladded with satellite 6-WC composites by using gas tungsten arc welding (GTAW) process. For this purpose, steel samples were coated with unreinforced and reinforced stellite (by 20, 30 and 40 wt.% WC). The cladded samples were evaluated by metallographic studies, microhardness measurement and X-ray diff...
در این تحقیق به بررسی ساختار میکروسکوپی و خواص سایش روکش استلایت 6 بر سطح فولاد زنگ نزن 316 بدون حضور و باحضور درصد های وزنی مختلف (10، 20 و 30) ذرات tic پرداخته شد. جهت اعمال روکش از فرایند جوشکاری قوسی تنگستن-گاز(tig) با سه حرارت ورودی مختلف و دو نوع جریان dcen معمولی و پالسی استفاده گردید. همچنین به منظور امکان سنجی رسوب مجدد ذرات ticحل شده نمونه ها عملیات حرارتی شدند. ریز ساختار روکش توسط م...