Journal: :journal of modern processes in manufacturing and production 0
hossein nouri hosseinabadi department of engineering, mechanical department, najafabad branch, islamic azad university, najafabad, iran masoud farahnakian department of engineering, mechanical department, najafabad branch, islamic azad university, najafabad, iran

nowadays the surface texturing has been widely recognized as a usable capability to improve the tribological systems. in this paper, ultrasonic assisted turning (uat) isperformed to create the micro textures on the flat faces. micro surface texturing ismade on the al7075-t6 by the uat in the face turning process. then, the influences of cutting speed feed, vibration direction and vibration ampl...

A. Akhbarizadeh K. Amini, S. Javadpour

Deep cryogenic heat treatment is assumed as a supplementary heat treatment performed on steels before the final tempering treatment to enhance the wear resistance and hardness of the steels. In this study, the effects of the deep cryogenic heat treatment on the wear behavior and corrosion resistance of the 1.2080 tool steel were studied using the wear testing machine and polarization and impeda...

The effects of applied load, sliding speed and sliding distance on the dry sliding wear behavior of aged Al-SiCp-Gr composites were investigated. The specimen were fabricated by stir-casting technique. The pin-on-disc wear testing machine was used to investigate the wear rate by design of experiments based on L27 using Taguchi technique. Sliding distance was the most important variable that inf...

M. K. Besharati Givi, H. Razmi, M. Emamy, J. Rassizadehghani, M. Alipour, S. Mirjavadi,

In this study the effect of Al–5Ti–1B grain refiner on the structural characteristics and wear properties of Al–12Zn–3Mg–2.5Cu alloy was investigated. The optimum amount for Ti containing grain refiners was selected as 2 wt.%. T6 heat treatment, (i.e. heating at 460 °C for 1 h before water quenching to room temperature and then aging at 120 °C for 24 h) was applied for all specimens before wear...

Journal: :international journal of iron & steel society of iran 2015
k. amini a. akhbarizadeh s. javadpour

deep cryogenic heat treatment is assumed as a supplementary heat treatment performed on steels before the finaltempering treatment to enhance the wear resistance and hardness of the steels. in this study, the effects of thedeep cryogenic heat treatment on the wear behavior and corrosion resistance of the 1.2080 tool steel were studiedusing the wear testing machine and polarization and impedance...

Journal: :international journal of iron & steel society of iran 2012
gh. zirehpour r. shoja razavi e. moayerifar

as the turbine industries need to manufacture turbine blades made of martensitic stainless steel aisi 420 with high toughness and wear resistance, local laser hardening has become more and more important. in this research, surface of the samples was initially hardened by high-power pulsed laser beam; then, optimum parameters of hardening were calculated and wear resistance of surface hardened s...

E. Moayerifar Gh. Zirehpour R. Shoja Razavi

As the turbine industries need to manufacture turbine blades made of martensitic stainless steel AISI 420 with high toughness and wear resistance, local laser hardening has become more and more important. In this research, surface of the samples was initially hardened by high-power pulsed laser beam; then, optimum parameters of hardening were calculated and wear resistance of surface hardened s...

2012
Joseph P. Hughes

.................................................................................................................... iv 1. Introduction .................................................................................................................. 1 2. Theory/Methodology for Wear in Prosthetic Implants ................................................ 3 2.1 Wear Mechanisms ..........

2005
Matthew R. Gevaert Martine LaBerge Jennifer M. Gordon John D. DesJardins

Background: The occurrence of multi-directional sliding motion between total knee replacement bearing surfaces is theorized to be a primary wear and failure mechanism of ultra-high molecular weight poly(ethylene) (UHMWPE). To better quantify the tribologic mechanisms of this cross-shear wear, the MAX-Shear wear-testing system was developed to evaluate candidate biomaterials under controlled con...

Journal: :Medical engineering & physics 2011
M A Strickland M R Dressler T Render M Browne M Taylor

Experimental testing is widely used to predict wear of total knee replacement (TKR) devices. Computational models cannot replace this essential in vitro testing, but they do have complementary strengths and capabilities, which make in silico models a valuable support tool for experimental wear investigations. For effective exploitation, these two separate domains should be closely corroborated ...