in this research, surface composite layers containing nano sized tib2, al2o3-tib2, zro2 and cnt particles have been fabricated on aluminum alloy substrates by friction stir processing. the effects of different processing variables such as number of passes and strengthening particle distribution, hardness, and wear properties of surface nanocomposite layers have been evaluated by electron micros...
The aim of the present study was to investigate the effect of quenching and tempering temperatures on the microstructure, mechanical properties and the wear characteristics of medium carbon-high chromium wear resistant steel. In addition, the dominant wear mechanisms were studied. For this purpose, austenitizing and tempering temperatures were selected in the ranges of 900- 1000 °C and 300- 500...
the aim of the present study was to investigate the effect of quenching and tempering temperatures on themicrostructure, mechanical properties and the wear characteristics of medium carbon-high chromium wear resistantsteel. in addition, the dominant wear mechanisms were studied. for this purpose, austenitizing and temperingtemperatures were selected in the ranges of 900- 1000 °c and 300- 500 °c...
objectives: dental composite wear in posterior restorations is a concern and is affected by different factors. this study was conducted to evaluate the effect of polishing and mechanical loads on wear of silorane-based and methyl methacrylate-based composites resins. materials and methods: of each dental composite (filtek p90 and filtek p60), 40 samples were fabricated in a polyethylene mold (4...
in this study, in order to investigate the effect of increasing the manganese content on microstructure and mechanical properties of high manganese austenitic steels, three alloys with successive increases in weight percentages of manganese (7.55, 13.1, and 16.5) and carbon (0.8 and 1.2) were cast in the presence of a constant amount of chromium (1.5 wt.%) and silica (0.6 wt.%). the samples exp...
polyvinyl ester green composites were synthesized with walnut shell powder (wsp) by in-situ polymerization technique. the green composites have been evaluated for mechanical properties such as tensile strength, tensile modulus and hardness. sliding wear loss, specific wear rate and coefficient of friction were investigated by using computerized pin-on–disc machine at normal applied loads of 20,...
In this research, surface composite layers containing nano sized TiB2, Al2O3-TiB2, ZrO2 and CNT particles have been fabricated on Aluminum alloy substrates by friction stir processing. The effects of different processing variables such as number of passes and strengthening particle distribution, hardness, and wear properties of surface nano...
Polymer matrix composites used in different industrial applications due to their enhanced mechanical properties and lightweight. However, these materials are subjected to friction and wear situations in some industrial and automobile applications. Therefore, there is a need to investigate the wear properties of polymer matrix composite materials. This article emphasizes the dry abrasive wear be...
Polyvinyl ester green composites were synthesized with walnut shell powder (WSP) by in-situ polymerization technique. The green composites have been evaluated for mechanical properties such as tensile strength, tensile modulus and hardness. Sliding wear loss, specific wear rate and coefficient of friction were investigated by using computerized pin-on–disc machine at normal applied loads of 20,...
In this research, surface composite layers containing nano sized TiB2, Al2O3-TiB2, ZrO2 and CNT particles have been fabricated on Aluminum alloy substrates by friction stir processing. The effects of different processing variables such as number of passes and strengthening particle distribution, hardness, and wear properties of surface nano...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید