The effects of applied load, sliding speed and sliding distance on the dry sliding wear behavior of aged Al-SiCp-Gr composites were investigated. The specimen were fabricated by stir-casting technique. The pin-on-disc wear testing machine was used to investigate the wear rate by design of experiments based on L27 using Taguchi technique. Sliding distance was the most important variable that inf...

Journal: :iranian journal of materials science and engineering 0
n. radhika amrita school of engineering, coimbatore,india r. raghu department of metallurgical engineering, psg college of technology, coimbatore-641004, india

functionally graded aluminium/zirconia metal matrix composite was fabricated using stir casting technique followed by horizontal centrifugal casting process and a hollow cylindrical functionally graded composite (150 x 150 x 16 mm) was obtained with centrifuging speed of 1200 rpm. the microstructural evaluation and hardness test was carried out on the outer and inner surface of the functionally...

In this study, small fraction of NiTi (5 wt%) was added to Yttria stabilized zirconia (YSZ) top coat to improve it sliding wear resistance. The measurement of width of wear tracks after wear tests under a 15 N load for 100 m sliding distances showed that the width of wear track in NiTi-YSZ coating is shorter than that in YSZ coating which depicts the higher wear resistance of NiTi-YSZ coa...

Journal: :journal of modern processes in manufacturing and production 0
hossein nouri hosseinabadi department of engineering, mechanical department, najafabad branch, islamic azad university, najafabad, iran masoud farahnakian department of engineering, mechanical department, najafabad branch, islamic azad university, najafabad, iran

nowadays the surface texturing has been widely recognized as a usable capability to improve the tribological systems. in this paper, ultrasonic assisted turning (uat) isperformed to create the micro textures on the flat faces. micro surface texturing ismade on the al7075-t6 by the uat in the face turning process. then, the influences of cutting speed feed, vibration direction and vibration ampl...

Journal: :iranian chemical communication 0
shahryar pashaei payame noor university

polyvinyl ester green composites were synthesized with walnut shell powder (wsp) by in-situ polymerization technique. the green composites have been evaluated for mechanical properties such as tensile strength, tensile modulus and hardness. sliding wear loss, specific wear rate and coefficient of friction were investigated by using computerized pin-on–disc machine at normal applied loads of 20,...

M. K. Besharati Givi, H. Razmi, M. Emamy, J. Rassizadehghani, M. Alipour, S. Mirjavadi,

In this study the effect of Al–5Ti–1B grain refiner on the structural characteristics and wear properties of Al–12Zn–3Mg–2.5Cu alloy was investigated. The optimum amount for Ti containing grain refiners was selected as 2 wt.%. T6 heat treatment, (i.e. heating at 460 °C for 1 h before water quenching to room temperature and then aging at 120 °C for 24 h) was applied for all specimens before wear...

In the current research work synthesis, characterization, mechanical and wear behavior of 5 and 10 wt. % of nano TiO2 particulates reinforced Al7075 alloy composites are inspected. The Al7075 alloy and nano TiO2 particle composites were provided by melt stir system. After the preparation, the prepared composites were analyzed by SEM, EDS, and XRD for inquiring the microstr...

2009
A. SAGBAS F. KAHRAMAN

Abrasive wear is defined wear due to hard particles or hard protuberances forced againts and moving along a solid surface. This defination encompasses several different mechanisms by which material removal occoures. The five types of wear are abrasive, adhesive, erosion, fatigue and fretting. The abrasive wear of polymeric materials is the interest and the subject of quite number of literature....

2017
G. Rasool James Weir

In this work, a study of the wear transition regimes was carried out for a pin-on-disk sliding couple, involving two steels of different hardness and Cr contents. Dry sliding wear behaviour of the more highly alloyed stainless steel was dominated by adhesive wear and tribo-oxidation at relatively low sliding speeds and by mixed and adhesive wear at high speeds and loads. In contrast, oxidative ...

A. Poladi, M. Zandrahimi,

Abstract: Austenitic stainless steels exhibit a low hardness and weak tribological properties. The wear behaviour of austenitic stainless steel AISI 316 was evaluated through the pin on disc tribological method. For investigating the effect of wear on the changes in microstructure and resistance to wear, optical microscopy and scanning electron microscope were used. The hardness of the worn...