نتایج جستجو برای: Nickel- based superalloy

تعداد نتایج: 2964286  

2010
Andrzej Nowotnik Jan Sieniawski

Experimental results on hot deformation and dynamic structural processes of nickel based alloy Inconel 718 are reviewed. The focus is the analysis of dynamic precipitation processes which operate during hot deformation of these materials at elevated temperatures. Hot compression tests were performed on the solution treated precipitation hardenable nickel based superalloy Inconel 718 at 720-1150...

2013
Maodong Kang Haiyan Gao Jun Wang Lishibao Ling Baode Sun

The dimensionless Niyama criterion was used to predict the formation of microporosity in nickel-based superalloy casting, which extended the model application from a simple plate casting to complex thin-wall superalloy casting. The physical characteristics of the superalloy were calculated by JMatPro software. The relation between the volume percentage of microporosity and the dimensionless Niy...

Journal: :SCIENTIA SINICA Technologica 2015

2015
Peng Zhang Qiang Zhu Gang Chen Heyong Qin Chuanjie Wang

The fatigue behavior of a nickel-base superalloy was investigated under total strain-controlled mode at high temperature. The fatigue life, cyclic stress response behavior and hysteresis loop of the superalloy were investigated under isothermal low cycle fatigue (LCF) conditions. The superalloy exhibited cyclic hardening and softening behaviors during the process of fatigue loading. The hystere...

Nickel base superalloy alloys are used in the manufacture of gas turbine engine components, which in use are exposed to high temperatures and corrosive environments. The platinum aluminide coatings described here have been developed to protect nickel base superalloy alloys from oxidation. In this study, the effect of cyclic oxidation, platinum layer thickness and aluminizing process on beha...

2017
D. Blavette A. Menand A. Bostel

Vari.ous methods available for the exploitation of atom-probe concentrat ion prof iles are discussed. T h e determinat ion of microstructure Parameters of a nickel base superalloy containing small precipitates is given a s an example.

2002
F. Tancret H. K. D. H. Bhadeshia

Models have been developed and used as tools to design a new `made to measure’ nickel base superalloy for power plant applications. In Part 1 Gaussian processes were used to model the mechanical properties of superalloys, and have been used as a basis for the design of a new Ni ± Cr ± W ± Al ± Ti ± Fe ± Si ± C ± B superalloy with desirable properties. In this part, an attempt has been made to d...

Journal: :international journal of iron & steel society of iran 2007
h. naffakh m. shamanian f. ashrafizadeh

the current work was carried out to characterize welding of aisi 310 austenitic stainless steel to inconel 657 nickel-chromium superalloy. the welds were produced using four types of filler materials; the nickel-based corresponding to inconel 82, inconel a, inconel 617 and austenitic stainless steels 310. of the two joints involved, this paper describes the choice of welding consumables for the...

2016
Amir Mostafaei Yashar Behnamian Yuval L. Krimer Erica L. Stevens Jing Li Luo Markus Chmielus

Powder bed binder jet printing (BJP) is an additive manufacturing method in which powder is deposited layer-by-layer and selectively joined in each layer with binder. The data presented here relates to the characterization of the as-received feedstock powder, BJP processing parameters, sample preparation and sintering profile ("Effect of solutionizing and aging on the microstructure and mechani...

نمودار تعداد نتایج جستجو در هر سال