the current study assesses the root causes of hydrogen blisters on low strength carbon steel equipment. for this purpose, some experiments including hardness test, non-destructive test (ndt), metallography, and fractograpghy are conducted. the microstructure of two blisters is assessed by means of optical microscopy and scanning electron microscopy (sem). the microstructural studies show that t...
recrystallization behavior of deep drawing low carbon steel sheets produced by mobarakeh steel plant
in the present work the recrystallization behavior of deep drawing grade al-killed low carbon steel sheets produced by mobarakeh steel plant (msp) has been studied. salt bath isothermal annealing has been applied to cold rolled samples and the resulted microstrucrures have been compared with the microstructure obtained from the box annealing process in msp. it is found that at 635 and 700ºc the...
friction-stir welding process is a novel method of solid state welding, which produces heat due to friction between the pin, the shoulder and the workpiece. this heat causes a paste area. shoulder pressure and pin spin cause edges integration and lead to welding. in this study, firstly, the feasibility of welding of steel sheet (en10130) with a thickness of 1.5mm has been tested by 58 experimen...
the unique properties of air-cooled bainitic steels have been described. a series of mn containing air-cooled bainitic steels invented by authors is presented in this paper: including low carbon granular bainitic steels, low carbon grain-boundary allotriomorphic ferrite/granular bainite duplex steels, medium and medium high carbon bainite/martensite duplex steel, and low carbon carbide free bai...
in the present study, the microstructure and mechanical properties of the dissimilar welding betweenastm a335 low alloy steel and er309l austenitic stainless steel were investigated using the gastungsten arc welding process. the welding of dissimilar materials between astm a335 low alloy steeland er309l austenitic stainless steel was found to have a significant effect on the microstructure when...
in the present work, deoxidation and refining of 316lvm steel (low carbon vacuum melted) during the vacuum induction melting process was studied. this grade of stainless steel is one of the most important materials in medical applications. vacuum deoxidation by carbon is the first stage of 316lvm stainless steel production process. in this stage, aluminum must be absent to avoid killing the c-o...
According to the characteristics of low-carbon steel pitting acoustic emission signal, one new characteristic analysis-WICA is proposed. The main idea of WICA is that based on the independent component analysis blind source separation technology as well as the wavelet transformation decomposition technology, proposed determines the low-carbon steel pitting source number according to the energy ...
The metallic low and intermediate level radioactive waste generally consists of carbon steel and stainless steels. The corrosion rate of carbon steel in deep groundwater is typically low, unless the water is very acidic or microbial activity in the environment is high. Therefore, the assessment of microbially induced corrosion of carbon steel in deep bedrock environment has become important for...
The unique properties of air-cooled bainitic steels have been described. A series of Mn containing air-cooled bainitic steels invented by authors is presented in this paper: including low carbon granular bainitic steels, low carbon grain-boundary allotriomorphic ferrite/granular bainite duplex steels, medium and medium high carbon bainite/martensite duplex steel, and low carbon carbide free bai...
This paper studied effects of ultrasonic treatment during the solidification process on structure formation of low carbon steel. Results showed that with ultrasonic treatment grains were refined and the steel ingot avoided the cast widmanstatten structure. When ultrasonic treatment was employed, pearlite was broken and the average length of pearlite was decreased from 550mm to 140mm. The corres...