Journal: :journal of nanostructures 2012
g. nabiyouni a. yousofnejad m. seraj s. farshad akhtarianfar d. ghanbari

hard magnetic srfe12o19 (srm) nanoparticles were synthesized by a facile sonochemical reaction. the magnetic nanoparticles were then added to acrylonitrile-butadiene-styrene, polystyrene, polycarbonate, and poly sulfone to make magnetic nanocomposites. the magnetic properties of the samples were also investigated using an alternating gradient force magnetometer. the strontium ferrite nanopartic...

A. Yousofnejad D. Ghanbari G. Nabiyouni, M. Seraj S. Farshad Akhtarianfar

Hard magnetic SrFe12O19 (SrM) nanoparticles were synthesized by a facile sonochemical reaction. The magnetic nanoparticles were then added to acrylonitrile-butadiene-styrene, polystyrene, polycarbonate, and poly sulfone to make magnetic nanocomposites. The magnetic properties of the samples were also investigated using an alternating gradient force magnetometer. The strontium ferrite nanop...

Journal: :journal of nanostructures 2013
gh. nabiyouni d. ghanbari a. yousofnejad m. seraj z. mirdamadian

magnetic cufe2o4 nanoparticles were synthesized by a facile microwave-assisted reaction between cu(no3)2 and fe(no3)3. the magnetic nanoparticles were added to starch to make magnetic polymeric nanocomposite. the nanoparticles and nanocomposites were characterized using x-ray diffraction and scanning electron microscopy. the magnetic properties of the samples were investigated using an alternat...

Abstract There are various methods to produce iron based nano crystalline magnetic alloys. Among these methods, mechanical alloying is one of the most important. In this research, nano crystalline Fe85Si10Ni5 soft magnetic alloy was synthesized by mechanical alloying. The effect of alloying time on phase constituents and magnetic properties of the produced powders was investigated, by X-ray di...

A. Yousofnejad D. Ghanbari Gh. Nabiyouni, M. Seraj Z. Mirdamadian

Magnetic CuFe2O4 nanoparticles were synthesized by a facile microwave-assisted reaction between Cu(NO3)2 and Fe(NO3)3. The magnetic nanoparticles were added to starch to make magnetic polymeric nanocomposite. The nanoparticles and nanocomposites were characterized using X-ray diffraction and scanning electron microscopy. The magn...

Journal: :journal of ultrafine grained and nanostructured materials 2014
mina salehi pirooz marashi maryam salehi reza ghannad

anodic aluminum oxide (aao) fabricated by two step anodization technique, is used as a template to synthesize feco nanowire arrays by ac electrodeposition technique. response surface methodology (rsm) is applied to design the experiments, fit an empirical model and optimize the conditions to achieve the best magnetic properties. the magnetic properties, pore dimensions, composition and structur...

خانجانی, علیرضا, قاسمی, علی, هادی, مرتضی,

In the present research NdFeB thin films coupled with buffer and capping layer of W were formed on Si/SiO2 substrate by means of RF magnetron sputtering. The system was annealed at vaccum at different temperatures of 450, 500, 550,. 600 and 650 °C Phase analysis was carried out by XRD and it was found that NdFeB was formed without the formation of any kind of secondary phase. The cross...

Journal: :journal of nanostructures 2012
r. jalajerdi f. gholamian h. shafie a. moraveji d. ghanbari

fe3o4 nanoparticles were synthesizedviaa simple chemical reaction between fecl2.4h2o and fe(no3)3.9h2o under nitrogen atmosphere at room temperature, and then nanoparticles were added to cellulose acetate (ca) polymer. the influence of nanoparticles on the thermal properties of ca polymeric matrix was studied using thermogravimetric analysis (tga). nanostructures were characterized by x-ray dif...

2002
X. J. Huang S. Y. Xu C. K. Ong Z. Yang

We systematically studied the dependencies of substrate temperature, laser fluence, deposition time, ambient gas pressure and laser frequency on the structural and magnetic properties of Nd–Fe–B thin films synthesized by pulsed-laser deposition at high substrate temperature Ts . A coercive force of 2.0–2.4 kOe was obtained on samples with a thickness of 70–90 nm and an average grain size of 50–...