نتایج جستجو برای: Abrasive granules

تعداد نتایج: 20539  

The already initiated studies are based on size and forms of abrasive grains, but few studies have addressed the influence on the concentration of abrasive grains. This research has been done to remove some of the mysteries associated in the media "abrasives" or "chips" used in vibratory and barrel finishing, this process included within the functions and characte...

Journal: :Machines 2021

The rotational motion of the medium granules under influence an impeller installed in bottom a cylindrical reservoir is considered. dependencies circulation velocity abrasive granules, as well dependence pressure flow on radius vibrating machine for different speeds rotation are obtained. Furthermore, velocities at various distances from center have been determined. amplitudes tangential and ra...

Journal: :The Journal of bone and joint surgery. British volume 1998
E W Morscher A Hefti U Aebi

One concern about the fixation of HA-coated implants is the possible disintegration of the surface, with the migration of HA granules into the joint space, producing third-body wear. We report a study of six revisions of HA-coated polyethylene RM cups at 9 to 14 years after successful primary arthroplasty. In all six hips, we found HA granules embedded in the articulating surface of the polyeth...

Journal: :Coatings 2021

The article presents the influence of applied method used for removing varnish coat on corrosion resistance car body sheet. tests were carried out samples prepared from factory-painted elements with pearlescent, metallized and acrylic varnish. Removal was performed by sandpaper grinding, glass bead blasting, disc blaze rapid stripping, soda blasting abrasive plastic granules. average thickness ...

2017
Ibrahim Sevim

If one of the surfaces which are in touch is rough and hard, it chips the other surface due to relative motion or touching forces. The wear is called two-body abrasive wear. If there are free abrasive particles between the two bodies, the wear is called three-body abrasive wear. The free abrasive particles may be external material dust or the remains of chipping. Usually, the wear starts as a t...

Journal: :تحقیقات مهندسی کشاورزی 0
مهدی کسرائی دانشجوی دکتری دانشگاه تربیت مدرس، دانشگاه شیراز علیرضا صبور روح اقدم استادیار دانشکده مهندسی، دانشگاه تربیت مدرس.

the plain carbon steel “ck45” has relatively well mechanical and metallurgical properties and low cost. the purpose of this research was the property evaluation of this steel on abrasive wear and impact for using in plows and other tillage tools. tillage tool should resist in abrasive wear and impact simultaneously. several heat treatments were done on specimens of this steel. a standard test d...

2014
Rishi Dev Joshi Gursewak Singh Brar Mithlesh Sharma

Magnetic abrasive machining is a surface finishing technique in which a magnetic field is used to force abrasive particles against the target surface. As such, finishing of conventionally inaccessible surfaces (e.g., the inside surface of a long curved pipe) is possible. The aim of this paper is to study maximum efficiency in terms of material removal rate with respect to magnetic flux density ...

2006
A. P. Harsha

Single and multipass two-body and three-body abrasive wear behaviour of various polyaryletherketone composites have been carried out by using a pin-on-disc machine and a rubber wheel abrasion test (RWAT) rig. Abrasive wear studies were conducted under different loads and sliding distances. Comparative wear performance of all the composites at different loads shows that specific wear rate (Ko) o...

2003
David Miles

Pliant abrasive media is transforming the way coating maintenance personnel approach offshore surface preparation. Pliant media users are often able to lower total job costs and provide higher quality surface preparation. 29(59,(:#2)#2))6+25(#0$,17(1$1&( Millions of dollars are being allocated toward the maintenance of offshore platforms with the goal to maximize oil production operations. A mo...

2017
A-Cheng Wang Ken-Chuan Cheng Kuan-Yu Chen Yan-Cherng Lin

Due to the fact that abrasive media can deform flexibly in abrasive flow machining (AFM) making this method easily to polish the complex holes and the curved surface of the hard machining shapes. Although abrasive media dominate the polishing behavior in AFM process, the mechanism of the abrasive media are not easy to understand because of the high viscous gels, therefore, many finishing works ...

نمودار تعداد نتایج جستجو در هر سال