A. Shafyei, H. R. Salimijazi, M. Akbarzadeh,

In the present study, CrN, TiN and (Ti, Cr)N coatings were deposited on D6 tool steel substrates. Physical and mechanical properties of coatings such as microstructure, thickness, phase composition, and hardness were evaluated. Phase compositions were studies by X-ray diffraction method. Mechanical properties were determined by nano-indentation technique. The friction and wear behaviour of the ...

Nitride coatings with excellent hardness and wear resistance have been deposited by physical vapor deposition (PVD) in recent years. For most applications, the load bearing and adhesion of coatings are very important and can determine the life and performance of the final components. In this study, CrN/CrAlN nanostructured coatings with different thicknesses and numberes of layers were deposite...

2004
Surya Prakash A. Poojari Harish C. Barshilia M. Surya Prakash K. S. Rajam

Nanocomposite coatings of TiN/a-C were prepared on tool steel substrates using a multitarget reactive DC magnetron sputtering process at various TiN layer thicknesses (0.6–2.8 nm). The a-C layer thickness was approximately 0.45 nm. Structural characterisation of the coatings was done by X-ray diffraction (XRD). Incorporation of an a-C phase in TiN matrix reduced crystallite size of the coatings...

2017
Wenquan Wang Wenmo Li Hongyong Xu

The strengthening hard phases TiN/C1-xNxTi were generated by in-situ solid-gas reaction in Ni-based composite coatings prepared using a plasma spray welding process to reinforce the wear resistance of the coatings. The microstructures and properties of the coatings were investigated. The results showed that the coatings mainly consisted of phases such as TiN, C1-xNxTi, TiC, etc. A small amount ...

A. Bahrami H. Sabet K. Amini,

Mo40 low-alloy steels are mostly used to produce industrial components such as crane wheels which are exposed to abrasive wear. However, during working conditions, their wear resistance is reduced after a while due to its low hardness. With increasing abrasive wear, the dimensions of components decrease and they need to be repaired for surface modification. In this regard, hard overlay coatings...

2016
Yiyong Wang Zhipeng Liang Junwei Zhang Zhe Ning Hui Jin

Ni-Co duplex coatings were cladded onto Cu to improve the antiwear properties of Cu products. Prior to laser cladding, n-Al₂O₃/Ni layers were introduced as interlayers between laser cladding coatings and Cu substrates to improve the laser absorptivity of these substrates and ensure defect-free laser cladding coatings. The structure and morphology of the coatings were characterized by scanning e...

Journal: :مهندسی متالورژی و مواد 0
زهرا انصاری مصطفی علیزاده عباس صادق زاده عطار

in this study, mixed metal oxides al2o3/mgo/tio2 coatings with al/mg/ti ratio of 5:1:3 and 2.5:3:4 were coated on aluminum by sol-gel method. the surface morphology, phase analysis, thermal behavior and the corrosion behavior of the al2o3/mgo/tio2 coatings were characterized by (sem), (xrd), (tg-dta) and potentiodynamic polarization test in 3.5 wt.% nacl solution. the results demonstrated that ...

  There are many factors such as voltages, duty cycle, pressure, temperatures and gas flux in coatings process that were effective in changing coatings characteristic. In this paper in plasma enhanced chemical vapor deposition (PECVD) technique, temperature and gas flux are two important variants that affecting the coatings structure and mechanical properties. All TiC coating deposited on a hot...

2012
N. W. Khun H. Zhang J. L. Yang E. Liu

The effect of wax-containing microcapsules incorporated in silicone composite coatings deposited on aluminum (Al) alloy substrates on the tribological performance of the coatings was systematically investigated. The wax-containing microcapsules were prepared via in situ polymerization. The tribological behavior of the composite coatings was evaluated using ball-on-disk tribological test. It was...

2017
Yixuan Wu Qiang Luo Jin Jiao Xianshun Wei Jun Shen Junwei Qiao

The wear behavior of two coatings (Fe49.7Cr18Mn1.9Mo7.4W1.6B15.2C3.8Si2.4 and Fe40Cr23Mo14C15B6Y2) sprayed by high-velocity air fuel technology was investigated through nanoscratch tests under ramping loads. Compared with the substrate, the Fe-based amorphous coatings exhibit lower penetration depth, higher elastic recovery, and lower wear volume, indicating the excellent wear resistance of the...