نتایج جستجو برای: eutectoid steel

تعداد نتایج: 81440  

2012

3 IMR KINKEN Research Highlights 2012 IMR KINKEN Research Highlights 2012 To reduce the fuel consumption by automobiles, medium carbon steels for forging parts, such as shafts and connecting rods, must be further strengthened. When carbide-forming elements such as Ti, Nb, and V, are alloyed with carbon steels, a fine dispersion of alloy carbides and large precipitation hardening can be achieved...

Journal: :Physical review letters 2007
E A Brener C Hüter D Pilipenko D E Temkin

Melting of a bicrystal along the grain boundary is discussed. A triple junction plays a crucial role in the velocity selection problem in this case. In some range of the parameters an entirely analytical solution of this problem is given. This allows us to present a transparent picture of the structure of the selection theory. We also discuss the selection problem in the case of the growth of a...

Journal: :Strojniški vestnik 2021

The work deals with the fabrication of a joint between AZ31 magnesium alloy and AW-6060 aluminium use Zn interlayer. layer was produced on surface an insert by diffusion bonding. then placed inside steel mould kept at room temperature. using compound casting filling liquid alloy, heated to 650 °C. microstructure bonding zone formed joined alloys analysed optical microscope scanning electron equ...

Journal: :Materials Characterization 2022

The effect of Si addition on the evolution bainitic transformation, carbon diffusion, carbide formation, and dislocation density in steel was investigated using in-situ high-energy X-ray diffraction (HEXRD). Alloys Fe-0.4C-1.7Mn (in wt%) with 1–4 wt% were austenitized at 1273 K then isothermally heat treated 573, 623, 673 K. According to HEXRD results, increasing content reduces transformation ...

2016
A. Scherf A. Kauffmann S. Kauffmann-Weiss T. Scherer X. Li F. Stein M. Heilmaier

Fe-Al alloys in the aluminium range of 55-65 at.% exhibit a lamellar microstructure of B2-ordered FeAl and triclinic FeAl2, which is caused by a eutectoid decomposition of the high-temperature Fe5Al8 phase, the so-called ∊ phase. The orientation relationship of FeAl and FeAl2 has previously been studied by Bastin et al. [J. Cryst. Growth (1978 ▸), 43, 745] and Hirata et al. [Philos. Mag. Lett. ...