2002
Fushuang Cui Alberto Sagüés

The corrosion performance of stainless steel clad reinforcing bar (SCR) was investigated. Corrosion potential of SCR in various alkaline media as a function of time was measured periodically and corrosion rates were estimated using Electrochemical Impedance Spectroscopy (EIS). At room temperature, SCR without cladding breaks was free of corrosion for up to one year in all the testing conditions...

2015
Kang Yuan Ru Lin Peng Xin-Hai Li Sten Johansson Yandong Wang Lin Peng

HVOF-sprayed CoNiCrAlYSi coatings were tested at 900 °C in a hot corrosion environment containing sodium-potassium sulphates. The HVOF spraying caused the typical splat-on-splat structure. The results after the hot corrosion testing showed that the corrosion preferentially occurred at the coating surface and the splat boundaries. The oxidation along the splat boundaries can isolate the splat fr...

1999
W. KAEMPFER M. BERNDT

The expense of repair and maintenance of private and public sewage systems in Germany runs to about 100 billion US $. This primarily affects concrete pipes and brickwork sewers. Approximately 40 per cent of the damage can be attributed to corrosion by biogenous sulfuric acid attack as a result of long flow periods and insufficient ventilation of waste water. The report deals with investigations...

Journal: :Journal of orthopaedic research : official publication of the Orthopaedic Research Society 2018
Anna Panagiotidou Timothy Cobb Jay Meswania John Skinner Alister Hart Fares Haddad Gordon Blunn

Wear and corrosion at the modular head-neck junction has been recognised to be a potential clinical concern, with multiple reports on adverse local tissue reactions and subsequent early failure of metal-on-metal hip replacements. Furthermore, reports on head-neck taper corrosion are also being described with conventional metal-on-polyethylene bearings. Manufacturing tolerances, surgical techniq...

2013
Jennifer Lynn

A surface hardening technique called “interstitial hardening” has been developed to introduce interstitial carbon atoms into stainless steel surfaces without the formation of carbides. Surface hardening of machine elements such as impellors or fasteners would improve performance regarding cavitation and galling resistance, and has intensified interest in this process. The interstitial hardening...

2016
Karin JACOBSON Johan CARLSON Philip LINDBLAD

Equipment and components made of plastics and composites are widely used in highly corrosive environments in the processing industry. Examples are the storage tanks, pumps and pipes for chemical transport and stacks in combustion plants. The demand for reliable nondestructive testing of plastic process equipment has increased significantly in recent years. Glass fiber reinforced plastics (GRP) ...

2011
Rohollah Ghasemi Inger Odnevall Wallinder

In this work, Slow Strain Rate Test (SSRT) testing, Light Optical Microscopy (LOM) and Scanning Electron Microscopy (SEM) were used to study the effect of microstructure, corrosive environments and cathodic polarisation on stress corrosion cracking (SCC) of two grades of high strength steels, Type A and Type B. Type A is manufactured by quench and tempered (Q&T) method. Type B, a normalize stee...

2016
Daniel F. Weyer Jeffrey E. Shield

Power District (NPPD) implemented an inspection program to determine the extent of condition for this type of widely used conductor. Other companies which have had related issues with similar types of corrosion have simply replaced their existing insignificant miles of conductor; however NPPD transmission system includes over 2000 miles of this particular conductor. Throughout 2012, many other ...

2016
Gaius Debi Eyu Geoffrey Will Willem Dekkers Jennifer MacLeod

The effect of potassium iodide (KI) and sodium nitrite (NaNO₂ inhibitor on the corrosion inhibition of mild steel in chloride bicarbonate solution has been studied using electrochemical techniques. Potentiodynamic polarisation data suggest that, when used in combination, KI and NaNO₂ function together to inhibit reactions at both the anode and the cathode, but predominantly anodic. KI/NO₂- conc...