نتایج جستجو برای: wear mechanism

تعداد نتایج: 590195  

Journal: :Friction 2021

Abstract Current three-body abrasive wear theories are based on a macroscale indentation process, and these claim that material cannot be achieved without damaging the hard mating surface. In this study, process of nano-abrasive system including single crystalline silicon substrate, an amorphous silica cluster, polyurethane pad, chemical mechanical polishing (CMP) is investigated via molecular ...

M. Salehi and A.S. Ayatollahi,

In this research the effect of volume and morphology of eutectic carbides on tribological behaviour of Ni-Hard 4 cast irons have been investigated. Therefore, as a result of the fact that the carbon content effects the carbides morphology of Ni-hard cast irons, the chemical compositions of five different specimens were kept constant with the exception of the carbon content, which was varied fro...

Journal: :The Journal of bone and joint surgery. British volume 1992
S M Jones I M Pinder C G Moran A J Malcolm

Isolated wear of the polyethylene tibial component led to failure in five of a series of 108 uncemented porous-coated knee replacements. The clinical features included pain, effusion and instability with progressive varus deformity. In all cases there was extensive wear on the medial side of the polyethylene surface of the prosthesis. The mechanism of such wear is complex, being due in part to ...

2017
Lei Chen Yaqiong Qi Bingjun Yu Linmao Qian

Fundamental understanding of tribochemical wear mechanism of oxide-free single crystalline silicon (without native oxide layer) is essential to optimize the process of ultra-precision surface manufacturing. Here, we report sliding speed-dependent nanowear of oxide-free silicon against SiO2 microspheres in air and in deionized water. When contact pressure is too low to induce Si yield, tribochem...

2018
Li Jiahong Kong Dejun

Cr-Ni coatings with the mass ratios of 17% Cr-83% Ni, 20% Cr-80% Ni and 24% Cr-76% Ni were fabricated on H13 hot work mould steel using a laser cladding (LC). The surface-interface morphologies, chemical elements, surface roughness and phase composition of the obtained Cr-Ni coatings were analysed using a scanning electron microscope (SEM), energy disperse spectroscopy (EDS), atomic force micro...

Journal: :Journal of the Japan Institute of Metals and Materials 1959

Journal: :Dental materials journal 2014
Mai Hara Yusuke Takuma Toru Sato Taku Koyama Masao Yoshinari

The wear performances of bovine tooth enamel (BTE) against translucent tetragonal zirconia polycrystals (TZP) compared to that of feldspar porcelain and the influence of surface treatments of translucent TZP were investigated by the two-body wear test. Translucent TZP and feldspar porcelain were used as hemisphere abrader specimens with a radius of curvature of 5 mm; flat BTE surfaces were used...

2017
Zhaolong Zhu Xiaolei Guo Bin Na Xingyu Liang

The effect of cutting parameters and tool parameters on cutting forces and tool wear were investigated in high density fiberboard (HDF) peripheral up-milling using toughened ceramic cutting tools. The results showed that whether at low speed cutting or high speed cutting, the tangential forces Ft and normal forces Fr increased slowly with the increase of cutting length. The tangential forces Ft...

2018
Junfeng Xiang Siqin Pang Lijing Xie Feinong Gao Xin Hu Jie Yi Fang Hu

The aim of this work is to analyze the micro mechanisms underlying the wear of macroscale tools during diamond machining of SiCp/Al6063 composites and to develop the mechanism-based diamond wear model in relation to the dominant wear behaviors. During drilling, high volume fraction SiCp/Al6063 composites containing Cu, the dominant wear mechanisms of diamond tool involve thermodynamically activ...