The cleavage fracture of a carbon structural steel is shown to deviate from what is typical of a ferritic matrix. This occurs at temperatures ranging from 150 to 20 C and affects the scatter of fracture toughness, and fractographic features. To explain the observed discrepancies a probabilistic model is developed by linking physical mechanisms of cleavage with continuum mechanics analysis appli...
Armour steel is a medium-carbon which widely used in military and defense industries owing to its ability protect from projectile bullet pressure. However, this armour still posses mechanical limitation aspect, thus it needed engineer for improvement. Therefore, the aim of research undergo properties engineering by using heat treatment method austempering within temperature variations 200, 250,...
The microstructure obtained as the weld cools from the liquid phase to ambient temperature is called the as–deposited or primary microstructure. Its major components include allotriomorphic ferrite, Widmanstätten ferrite, and acicular ferrite (Fig. 1). There may also be some martensite, retained austenite or degenerate pearlite. These latter phases occur in very small fractions, and are known b...
In this research (using induction furnace process) nodular iron with three different percentages of copper (residual, 0.5% and 1,2%) was obtained. Chemical analysis was performed by mass spectrometry and microstructures were characterized by Optical Microscopy (ASTM E3) and Scanning Electron Microscopy (SEM). The study of mechanical behavior was carried out in a mechanical test machine (ASTM E8...
نمودار تعداد نتایج جستجو در هر سال
با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید