High-strength steels, despite their excellent mechanical properties in normal conditions, can be susceptible to hydrogen embrittlement. Due the service loads or residual stresses, migrates within component and accumulates regions where highest tensile hydrostatic stress occurs. As a consequence, brittle failure occur even if initial mean concentration is lower than critical value. The availabil...