Uniform nanostructure coating of TiO2 was prepared on 316L stainless steel by sol-gel method using Tetra-n-Butyle Titanat (TBT) as alkoxide material. 316L specimens were coated with the mentioned sol by dip coating method. The influences of preparation condition, pH of sol on TiO2 nanostructure coating were investigated. Their structural properties were examined at var...
To solve crack problems, some coupled methods have been developed in recent years. Most of these methods have some shortcomings such as the need for a transition region. The finite element and enriched element free Galerkin methods are widely used for this class of problems. In order to take the advantages of these methods while avoiding the disadvantages, it is essential to follow solution app...
The dentin-enamel junction (DEJ), which is the interfacial region between the dentin and outer enamel coating in teeth, is known for its unique biomechanical properties that provide a crack-arrest barrier for flaws formed in the brittle enamel1. In this work, we re-examine how cracks propagate in the proximity of the DEJ, and specifically quantify, using interfacial fracture mechanics, the frac...
The strength and ductility of microcrystalline and nanocrystalline tungstsen carbide–cobalt (WC–Co) cermets have been evaluated by employing a stored energy Kolsky bar apparatus, high-speed photography and digital image correlation. The test specimens were thin-walled tubular Al7075-T6 substrates 250 μm thick, coated with a 300 μm thick microcrystalline or nanocrystalline WC–Co layer with an av...
Thisstudy presents axially forced vibration of a cracked nanorod under harmonic external dynamically load. In constitutive equation of problem, the nonlocal elasticity theory is used. The Crack is modelled as an axial spring in the crack section. In the axial spring model, the nonrod separates two sub-nanorods and the flexibility of the axial spring represents the effect of the crack. Boundary ...
The improvement and mechanism of the fatigue resistance of TC21 high-strength titanium alloy with a high velocity oxygen fuel (HVOF) sprayed WC-17Co coating was investigated. X-ray diffraction (XRD) and the corresponding stress measurement instrument, a surface roughness tester, a micro-hardness tester, and a scanning electron microscope (SEM) were used to determine the properties of the HVOF W...
Nanostructured alumina thin films were coated on stainless steel by Sol-Gel dip coating method. In order to prevent crack formation, Al2O3 films were kept in a solvent bath immediately after coating to reduce the rate of drying. Effects of calcination temperature and withdrawal speed on structural properties were analyzed using XRD and SEM. Topography and thickness of coat...
ÐOngoing research is reported aimed at improving bio®xation through the use of bioactive glass coatings on Ti-based implant alloys. The optimized processing conditions for coating with one promising bioactive glass composition are discussed, and the stress corrosion crack growth behavior in a simulated human physiological environment is presented. This glass can be successfully used to coat Ti ...
Zinc coating is formed by the heterogeneous assembly of the Γ, Γ1, δ, ζ and η phases whose mechanical properties greatly differ from each other. Thermal strains resulting from large differences between thermal expansion coefficients are partially relaxed by the formation of a crack network. In order to model this phenomenon, initial hardness, thermal expansion coefficient αi and toughness (KIC)...