As an advanced manufacturing technology which has been developed rapidly in recent years, high speed machining is widely applied in many industries. The chip formation during high speed machining is a complicated material deformation and removing process. In research area of high speed machining, the prediction of chip morphology is a hot and difficult topic. A finite element method based on th...
The 316L stainless steel has been widely used in both artificial knee and hip joints in biomedical applications. The average lifetime of artificial hip joints is about 10 years due to aseptic loosening of the femoral stem attributed to polymeric wear debris; however, there is a steadily increasing demand from younger osteoarthritis patients aged between 15 and 40 years for a longer lasting join...
Band contrast (BC) is a qualitative measure of electron back-scattered diffraction (EBSD), which is derived from the intensity of the Kikuchi bands. The BC is dependent upon several factors including scanning electron microscope measurement parameters, EBSD camera setup, and the specimen itself (lattice defect and grain orientation). In this study, the effective factors for BC variations and th...
In this study, two-dimensional finite element modeling was used to study the simultaneous effect of the cell shape and regular cell distribution on the anisotropy of the elastic properties of 316L stainless steel foam. In this way, the uniaxial compressive stress-strain curve was predicted using a geometric model and fully solid 316L stainless steel. The results showed that the elastic tangent ...
In modern history, metals have been used as implants since more than 100 years ago when Lane first introduced metal plate for bone fracture fixation in 1895 (Lane, 1895). In the early development, metal implants faced corrosion and insufficient strength problems (Lambotte, 1909, Sherman, 1912). Shortly after the introduction of the 18-8 stainless steel in 1920s, which has had far-superior corro...
There are many industries where austenitic stainless steel needs to be welded specially in power generation industries. Unfortunately the austenitic stainless welding has several fabrication and metallurgical drawbacks when welded by using conventional fusion welding methods, which can often leads to in-service failure. The most pronounced fabrication faults are hot cracks due to inadvertent us...
Molten LiCl-KCl salt and liquid cadmium are proposed as the electrolyte reactive cathode for electrorefining of spent nuclear fuels, but they can be corrosive to structural alloys. The down-selection existing materials through corrosion testing is necessary ensure longevity electrorefiner vessel electrode assemblies. Haynes C276, Inconel 600, AISI 316L stainless steel, 42CrMo low-alloy steel we...
In this investigation, Ti/TiN nanolayer and TiN single layer coatings were coated on substrate of AISI 316L stainless steel by applying physical vapor deposition (PVD) using the type of cathodic arc evaporation (CAE). The evaluation of microstructure were carried out using x-ray diffraction (XRD), nanoindentation, atomic force microscopy (AFM) as well as scanning electron microscopy (SEM). Pola...