2012
Ram S. Mohan Radovan Kovacevic Raju Damarla

\nG ABSTRACT An abrasive waterjet nozzle wear monitoring and compensating mechanism using the frequency domain.acoustic signals geneiated by the jet exiting the nozzle, as input, is prbposed. An artificial neural network which forms the critical iart of this system is developed using the _back-propagatlon algorithm. The trained network is capable of determining the nozzle diameter corresponding...

2016
Qian Zhao Yunhong Liang Zhihui Zhang Xiujuan Li Luquan Ren

B4C ceramic particulate–reinforced Al 5083 matrix composite with various B4C content was fabricated successfully via hot-press sintering under Argon atmosphere. B4C particles presented relative high wettability, bonding strength and symmetrical distribution in the Al 5083 matrix. The hardness value, friction coefficient and wear resistance of the composite were higher than those of the Al 5083 ...

2010
Daniel E. Saloni Richard L. Lemaster Steven D. Jackson

Wood processing industries have continuously developed and improved technologies and processes to transform wood to obtain better final product quality and thus increase profits. Abrasive machining is one of the most important of these processes and therefore merits special attention and study. The objective of this work was to evaluate and demonstrate a process monitoring system for use in the...

Journal: :Journal of the Japan Society of Precision Engineering 1969

2012
Nándor Békési

In order to properly model the friction and wear of elastomer materials, it is essential to understand some specific mechanical and tribological features. Mechanical characteristics of elastomer materials are different from those of metals and other relatively hard materials. Elastomers can bear large deformations, the stress-strain curves are non-linear, time and temperature dependent. When th...

Journal: :journal of modern processes in manufacturing and production 2014
hassan gheisari

in this study; utilizing the elastic matrix ball has higher processing efficiency and better superficial quality than traditionalgrinding. the diversity of elastic abrasive tool characteristics contact with bend surface results in irregular wear abrasion,and abrasive tool machining status gets complicated. there is no theoretical interpretation of parameters affecting the grinding accuracy. bec...

2016
Shili Shu Hongyu Yang Cunzhu Tong Feng Qiu

Metal matrix composites reinforced with ceramic particles have become the most attractive material in the research and development of new materials for thermal management applications. In this work, 40-60 vol. % TiCx-TiB₂/Al composites were successfully fabricated by the method of combustion synthesis and hot press consolidation in an Al-Ti-B₄C system. The effect of the TiCx-TiB₂ content on the...

2009
M. A. Masen

A recent development in sheet metal forming industry is the application of tailored blanks: blanks prepared from separate pieces of sheet material, welded together prior to the forming process. The pieces of sheet material can have different properties, enabling weight reduction of components, corrosion resistance using cathodic protection or the possibility to create local weak spots, resultin...

2012
Radomir Slavkovic Zvonimir Jugovic Snezana Dragicevic Slavko Arsovski Aleksandar Jovicic Vladimir Slavkovic

Abrasive wear is one of the prime and mostly costly causes of secondary failure in the design and operation of mechanical machines and equipment. Wear limits must be known and measured to assure quality and durability of products by an experimental process to determine an optimum material composition. The development of wear monitoring systems for industrial processes is well recognised in the ...

2012
E. OLEJNIK

E. Olejnik, A. Janas, B. Grabowska, M. Kawalec, AGH University of Science and Technology, Faculty of Foundry Engineering, Krakow, Poland Casting technology was applied and research was carried out on two alloys based on the Ni3Al phase with variable carbon content of 0,2 and 1,25 wt. % C, respectively. Resistance to abrasive wear, friction coeffi cient and Vickers microhardness were determined....