The purpose of this study was to evaluate the flexural strength of a direct composite, for indirect application, that received heat treatment, with or without investment. One indirect composite was used for comparison. For determination of the heat treatment temperature, thermogravimetric analysis (TGA) and differential scanning calorimetry (DSC) were performed, considering the initial weight l...
thermal barrier coatings (tbcs) are used to provide thermal insulation to the hot section components of gas turbines in order to enhance the operating temperature and turbine efficiency. hot corrosion and thermal shocks are the main destructive factors in tbcs which comes as a result of oxygen and molten salt diffusion into the coating. in this thesis atmospheric plasma spraying was used to dep...
OBJECTIVE This experimental in vitro study compared marginal adaptation of indirect composite, glass-ceramic inlays and direct composite. MATERIALS AND METHODS Seventy-five recently extracted human molars were randomly divided into three groups (n=25) and mesio-occluso-distal cavities with the same dimensions were prepared in the teeth. Indirect composite and glass-ceramic inlays were fabrica...
We present a novel method to produce a PMMA-quantum-dot (QD) composite fabricated by pre-polymerization of PMMA and dispersing commercially available colloidal semiconductor QDs. The QDs are stabilized in rapidly formed oligomer matrices, and the complete polymerization of the PMMA-QD composite is achieved by commonly used polymerization. The properties of the PMMA-QD composite are measured and...
AIM The aim of this report is to present five-year follow-ups of two different applications for the use of direct laminate resin-based composite veneers to improve esthetics. BACKGROUND Defects in the maxillary anterior teeth, such as enamel hypoplasia and peg lateral, can present esthetic challenges. Furthermore, a treatment plan that can be completed in a single appointment is highly desira...
In this study, aluminium composite foams reinforced by different volume fractions of SiC particles as reinforcement and stabilizing agent were fabricated with the direct foaming route of melt using different contents of CaCO3 as foaming agent. The density of produced foams were measured to be from 0.38 to 0.68 g/cm3. The microstructural features and compressive properties of the AA356/SiCp comp...
Background: Modern restorative dentistry offers many methods of restoring the carious teeth. The advancements in adhesive dentistry have brought significant changes in the treatment of caries. Dental composite formulations have been continuously evolving ever since BISGMA was introduced to dentistry by Boven in 1962. The composite materials can be divided into direct and indirect resin composit...
direct composite resin restorations are widely used and the impact of different storage temperatures on composites is not well understood. the purpose of this study was to evaluate the microtensile bond strength of composite to dentin after different pre-curing temperatures.occlusal surfaces of 44 human molars were ground with diamond burs under water coolant and polished with 600 grit silicon ...
background: the purpose of this in vitro study was to evaluate surface discoloration of three microhybrid composite resins (esthet•x hd, clearfi l ap-x, gradia direct) and fi ve nanohybrid composite resins (ceram•x, gc kalore, g-aenial, grandio, grandioso), after staining and bleaching procedures. materials and methods: the composite resins were polymerized with a curing light (celalux ii, voco...