TiO2 nanoparticles were synthesized from titanium isopropoxide by a simple peptization method using sulfuric, nitric, and acetic acids. The effect of peptizing acid on physicochemical and photocatalytic properties of TiO2 powders was studied. The structural properties of synthesized TiO2 powders were analyzed by using XRD, TEM, N2-physisorption, Raman, DR UV-vis, FTIR, and X-ray photoelectron s...
The structural stability of some nanostructured titanates was investigated in terms of their subsequent processing and possible applications. With the aim to investigate their mechanochemical stability, we applied high-energy ball milling and studied the resulting induced phase transitions. Hydrogen titanates with two different morphologies, microcrystals and nanotubes, were taken into consider...
The photocatalytic behavior of titania coatings is largely determined by their crystalline structure. Depending on deposition conditions, though, titania may form amorphous, brookite, anatase or rutile structures, with anatase or anatase/rutile mixed phase structures showing the highest levels of activity. Anatase is activated by UV light and, consequently, there is a great deal of interest in ...
Anatase/rutile mixed titania nanotubes (TiO2 NTs) precipitated with gold nanoparticles (Au NPs), i.e. Au/TiO2, have been synthesized and investigated on visible photocatalysis properties. A deposition-precipitation (DP) method was adopted to reduce the gold precursor to Au NPs within the preformed TiO2 NTs by the emulsion electrospinning technique. The optimal visible photocatalytic activity wa...
AUTHOR EMAIL ADDRESS ([email protected]) RECEIVED DATE (to be automatically inserted after your manuscript is accepted if required according to the journal that you are submitting your paper to) TITLE RUNNING HEAD 'High temperature stable anatase TiO 2 ' CORRESPONDING AUTHOR FOOTNOTE *[email protected] 2 ABSTRACT: In the absence of a dopant or precursor modification, anatase to rutile tra...
Anatase TiO2 nanoparticles with average particle size ranging between 12 and 23 nm were synthesized by metalorganic chemical vapor deposition. The structure and particle size were determined by x-ray diffraction and transmission electron microscopy. The specific surface areas were measured by Brunauer-Emmett-Teller and ranged from 65 to 125 m2/g. The size effects on the stability of TiO2 in the...
Anatase TiO2 nanoparticles with exposed {001} facets were synthesized from Ti powder via a sequential hydrothermal reaction process. At the first-step hydrothermal reaction, H-titanate nanowires were obtained in NaOH solution with Ti powder, and at second-step hydrothermal reaction, anatase TiO2 nanoparticles with exposed {001} facets were formed in NH4F solution. If the second-step hydrotherma...
TiO2-based nanofibers were synthesized using a sol-gel method and electrospinning technique. The as-spun composite fibers were heat-treated at different temperatures (500°C, 550°C, 600°C, and 650°C) and atmospheres (ammonia and nitrogen) for 4 h. The fibers had diameters of 50 to 200 nm and mainly featured anatase and rutile phases. The anatase phase decreased and the rutile phase increased wit...
Detailed EPR investigations on as-grown and annealed TiO2 nanoparticles in the anatase and rutile phases were carried out at X-band (9.6 GHz) at 77, 120-300 K and at 236 GHz at 292 K. The analysis of EPR data for as-grown and annealed anatase and rutile samples revealed the presence of several paramagnetic centers: Ti3+, O-, adsorbed oxygen (O2-) and oxygen vacancies. On the other hand, in as-g...