J S Tiley G B Viswanathan A Shiveley M Tschopp R Srinivasan R Banerjee H L Fraser

Precipitates of the ordered L1(2) gamma' phase (dispersed in the face-centered cubic or FCC gamma matrix) were imaged in Rene 88 DT, a commercial multicomponent Ni-based superalloy, using energy-filtered transmission electron microscopy (EFTEM). Imaging was performed using the Cr, Co, Ni, Ti and Al elemental L-absorption edges in the energy loss spectrum. Manual and automated segmentation proce...

2010
J. S. Tiley G. B. Viswanathan A. Shiveley M. Tschopp R. Srinivasan R. Banerjee H. L. Fraser

Precipitates of the ordered L12 ’ phase (dispersed in the face-centered cubic or FCC  matrix) were imaged in Rene 88 DT, a commercial multicomponent Ni-based superalloy, using energy filtered transmission electron microscopy (EFTEM). Imaging was performed using the Cr, Co, Ni, Ti and Al elemental L-edges in the energy loss spectrum. Manual and automated segmentation procedures were utilized f...