AIM The aim of this study was to investigate the influence of three different thicknesses of In-Ceram core on the load at fracture of all-ceramic crowns. METHODS AND MATERIALS Thirty standardized crown-shaped nickel-chromium alloy dies were fabricated using a milling machine. Twenty dies were prepared with a 1 mm shoulder for Groups A and B. The only difference in the ten dies used for Group ...
OBJECTIVE The present study is the second part of an investigation of strength, fracture toughness and microstructure of nine all-ceramic materials. In the present study, DC Zirkon, an experimental yttria partially stabilized zirconia, In-Ceram Zirconia slip and In-Ceram Zirconia dry-pressed were compared. METHODS Strength was appraised on ten bar-shaped specimens for each material (20 x 4 x ...
The coefficient of thermal expansion of core and veneer porcelains for all ceramic crowns must be compatible to prevent formation of stresses during the firing cycles. The purpose of this study was to use a thermal shock test to evaluate the crazing resistance of six all-ceramic crown systems. The systems tested were: Vita In-Ceram, Vita Hi-Ceram, Dicor veneered with Vitadur N, magnesia core ve...
Recension av: lnput & Output. The Process of Fieldwork, Archiving and Research in Folklore. Ed. by Ulrika Wolf-Knuts collaboration with Anders Salomonsson et al. Turku 2001. (NNF publication 10.) 191 s.
Objective: In this study, the effects of ceramic, chromium-nickel (Cr-Ni) and ceramic opaque sinterized on chromium-nickel (Cr-Ni+opaque) post-core materials and different colored (opaque white, white, yellow and brown) cements on final color of all-ceramics materials (In-Ceram, IPS Empress and IPS Empress II) were investigated. Material and Methods: Three groups of post-cores (ceramic, Cr-Ni a...
The aim of this study was to compare the in vitro caries inhibition of various resin-based materials. Class V cavities were prepared in twenty-five freshly extracted human premolar teeth which were then restored with glass-ionomer cement (Chemfill II), compomer (Compoglass F, Dyract AP) and composite resin (Tetric Ceram and Z 100). The teeth were submerged in an acid gel for 6 weeks. Each speci...
Marginal Fit Metal-Ceramic and In-Ceram Single Crown Cement retained in Implant-supported Abutments.
INTRODUCTION This study evaluated the cervical fit of cemented metal-ceramic and In-Ceram implant-supported crowns, before and after the cementing procedure. MATERIALS AND METHODS Twenty crowns cemented on implant abutments are divided into two groups (n = 10): Group 1 -cemented metal-ceramic crowns and group 2 - cemented In-Ceram crowns. The marginal adaptations before and after cementation ...