نتایج جستجو برای: meso porous glass ceramic

تعداد نتایج: 147657  

2018
Yong-Seok Jang Hyeong-Rok Noh Min-Ho Lee Myung-Jin Lim Tae-Sung Bae

This study was performed to evaluate the effect of a lithium-disilicate spray-liner application on both the bond strength between zirconia cores and heat-pressed lithium-disilicate glass-ceramic veneers, and the fracture strength of all-ceramic zirconia crowns. A lithium-disilicate reinforced liner was applied on the surface of a zirconia core and lithium-disilicate glass-ceramic was veneered o...

2013
V.Ranjith Kumar

Stringent emission regulations around the world necessitate the use of high-efficiency catalytic converters in vehicle exhaust systems. Experimental studies are more expensive than computational studies. Also using computational techniques allows one to obtain all the required data for the Catalytic Converter, some of which could not be measured. In the present work, Geometric modeling ceramic ...

2015
Wolfram Höland Marcel Schweiger Marc Dittmer Christian Ritzberger

The controlled precipitation of strontium fluoroapatite crystals was studied in four base glass compositions derived from the SiO2-Al2O3-Y2O3-SrO-Na2O-K2O/Rb2O/Cs2O-P2O5-F system. The crystal phase formation of these glasses and the main properties of the glass-ceramics, such as thermal and optical properties and radiopacity were compared with a fifth, a reference glass-ceramic. The reference g...

Journal: :Brazilian oral research 2015
Aurealice Rosa Maria Martins Valéria Bisinoto Gotti Marcos Massao Shimano Gilberto Antônio Borges Luciano de Souza Gonçalves

This study evaluated the influence of an alternative surface treatment on the microshear bond strength (μsbs) of zirconia-based ceramic. Thirty-five zirconia disks were assigned to five groups according to the following treatments: Control (CO), glass and silane were not applied to the zirconia surface; G1, air blasted with 100μm glass beads + glaze + silane; G2, a gel containing 15% (by weight...

2017
Eric Denes Guislaine Barrière Evelyne Poli Guillaume Lévêque

We read with interest the review published by Baino et al. (2015) about bioceramics and scaffolds. We would like to add some information as we produce a porous alumina ceramic (CERAMIL ®) which present almost all the criteria that characterize an ideal scaffold as presented in table 1 of the article. Converse to the assertion that porous alumina is only used in the fabrication of orbital implan...

2008

High-strength all-ceramic systems for fixed partial dentures (FPDs) is gaining popularity as an alternative to the well established metal-ceramic FPDs. Several new framework materials and technique such as lithium disilicate, aluminum oxide and yttrium tetragonal zirconia polycrystal have been developed with improved strength, marginal discrepancy and esthetics. Since not every all-ceramic syst...

2014
G. Bayrak

In this study, production possibility of glass and glass-ceramic produced from granite was investigated. The composition of granite based glass bath mixture was 50 wt% granite, 25 wt% dolomite and 25 wt% sodium carbonate. Composition that was grounded and mixed in a ball mill for 2 h was melted at 1500 ◦C for 1 h. Glass samples were heat treated for crystallization to produce glass-ceramic mate...

2016
José S. Moya Arturo Martínez Roberto López-Píriz Francisco Guitián Luis A. Díaz Leticia Esteban-Tejeda Belén Cabal Federico Sket Elisa Fernández-García Antoni P. Tomsia Ramón Torrecillas

Bacterial and fungal infections remain a major clinical challenge. Implant infections very often require complicated revision procedures that are troublesome to patients and costly to the healthcare system. Innovative approaches to tackle infections are urgently needed. We investigated the histological response of novel free P2O5 glass-ceramic rods implanted in the jaws of beagle dogs. Due to t...

Journal: :Clinical oral implants research 2007
Bjarni E Pjetursson Irena Sailer Marcel Zwahlen Christoph H F Hämmerle

OBJECTIVES The objective of this systematic review was to assess the 5-year survival rates of all-ceramic single crowns and to compare it with the survival rates of metal-ceramic crowns and to describe the incidence of biological and technical complications. METHODS An electronic Medline and Dental Global Publication Research System search complemented by manual searching was conducted to ide...

Macor coatings on 316 alloys substrates were prepared by plasma spraying. The crystallization temperature, thermal expansion coefficient of mica glass-ceramic were at 900ºC and 40× 10−7/◦C respectively. The microhardness of obtained glass-ceramic coating was 6.8GPa and the coefficient friction was 0.98 . 

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید