ژورنال: سلامت و محیط زیست 2015
جعفری منصوریان, حسین , حسینی, علیرضا, علیزاده, مصطفی, محوی, امیرحسین, ملکوتیان, محمد,

Background and Objective: Phenol and phenol derivatives in industrial wastewater are among the pollutants with priorities. The high cost and low efficiency of some routine treatment processes of industrial wastewater has limited their use. One of the new methods under consideration is, nowadays, adsorption using carbon nanotubes. This study was conducted in order to evaluate the application of ...

2002
T. Dürkop T. Brintlinger M. S. Fuhrer

The electron transport properties of a very long (20 micron) CVD-grown nanotube are reported. In this device the transport is dominated by intrinsic scattering processes at room temperature. The room temperature hole mobility is 20,000 cm/Vs, exceeding that of technologically-relevant semiconductors. The mobility increases with decreasing temperature, and is estimated to be greater than 180,000...

Journal: :Transactions of the Japan Society of Mechanical Engineers Series A 2011

Journal: :International Journal of Current Research in Science, Engineering & Technology 2018

Electroless composite coatings used for achieving of high hardness, lubrication properties, non-stick surface, abrasive coating applications that by impregnation of soft and hard particles into Ni matrix. Electroless Nickel-phosphorous coatings properties and performance is greatly affected by the amount of phosphorus in them. The phosphor in this coating usually varies from 1 to 13 percent. In...

2005
P. Kim J. Yi

Mesoporous Ni–alumina catalysts (Ni–alumina-pre and Ni–alumina-post) were synthesized by one-step sol–gel method using micelle complex comprising lauric acid and nickel ion as a template with metal source and using aluminum sec-butoxide as an aluminum source. The Ni–alumina catalysts showed relatively high surface areas (303 m/g for Ni–alumina-pre and 331 m/g for Ni–alumina-post) and narrow por...

Electroless composite coatings used for achieving of high hardness, lubrication properties, non-stick surface, abrasive coating applications that by impregnation of soft and hard particles into Ni matrix. Electroless Nickel-phosphorous coatings properties and performance is greatly affected by the amount of phosphorus in them. The phosphor in this coating usually varies from 1 to 13 percent. In...