نتایج جستجو برای: vacuum brazing

تعداد نتایج: 47874  

Journal: :QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY 1996

Journal: :Journal of Materials Research and Technology 2020

2012
R. Kalaivanan R. Rathnasamy

This paper investigates the experimental program on the study of heat transfer characteristics in micro-channels. The two test sections used are of 47 and 50 micro-channels in rectangular cross-section of equivalent diameters 387 and 327 μm respectively. Each channel of length 192 mm is fabricated on a 304 stainless steel substrate (230 mm x 160 mm x 1.6 mm) by photo chemical etching process. C...

2016
S. GANGADHARAN

Brazing of an austenitic-martensitic stainless steel (AMSS) with pure silver was carried out at 1053 K, 1073 K, and 1093 K (780 C, 800 C, and 820 C) with Ag-27Cu-5Sn (wt pct) as brazing filler material (BFM). Wettability of the liquid BFM over base AMSS surface was found to be poor. Application of nickel coating to the steel was observed to enhance the wettability and to enable the formation of...

Journal: :International Journal of Lightweight Materials and Manufacture 2021

Journal: :Metallurgical and Materials Transactions 2021

Abstract Brazing is a crucial joining technology in industries where nickel-superalloy components must be joined. Nickel-based brazing filler metals are extensively employed, possessing excellent mechanical properties, corrosion resistance, and retained strength at elevated temperatures. To function as metal, the alloy melting point reduced to below that of materials being joined, but addition ...

E Heshmat Dehkordi M.E Bajgholi

Both Zirconium-based alloys and 321stainless steel are widely used as engineering alloys due to their good mechanical properties. Conventional fusion welding techniques for Zr alloys and stainless steel are not feasible due to the formation of brittle intermetallic compounds such as (Zr3Fe, ZrFe2 and Zr2Fe) and corrosion cracking. Brazing is one of the most wide...

Amelzadeh, M. , Mirsalehi, S. E.,

Nowadays, cemented carbides-steels joints by brazing method are taken into consideration. One of the problems of these joints is the creation residual stresses that can reduce it with choose correct parameters of brazing. In this study, Silver base alloy filler containing copper, zinc and cadmium have been used in temperature 780°C and the effect of time parameter 5, 10 and 15 minutes on micros...

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید