In this study, the calcined coal gangue was mixed with Al powder at different mass fractions (5wt%〜35wt%). After being pressed 80MPa and sintered 1200°C for 2h, gangue/Al cermet material obtained. The phase composition, microstructure mechanical properties of were studied. results show that main components prepared materials are Al, mullite, AlN, alumina silicon. With increase powder, hardness ...