نتایج جستجو برای: coater

تعداد نتایج: 218  

This paper deals with the design and fabrication of a quartz-crystal resonator used in a thickness-monitor unit, measuring film thickness in a film-depositing system. A purpose-grown quartz crystal is cut to form the desired wafer. Two gold electrodes are deposited on both surfaces of the wafer to provide electrical contacts. The resonance frequency of the resonator, at room temperature, and th...

2012
Sujit Banerjee Tuan Le R. Daniel Haynes James E. Bradbury

ß-Cyclodextrin (ß-CD) solubilizes stickies from deinked pulp, commercial adhesive formulations, or magazine inserts, which demonstrates its potential as a washing aid. A new test to simulate coater scratches is described; it involves scraping the test paper sample across the surface of a thin layer chromatography plate and measuring the degree of scratching on the plate. Scratching was signific...

2014
Muhamad Saipul Fakir Azzuliani Supangat Khaulah Sulaiman

In this study, the spin coating of template-assisted method is used to synthesize poly[2,7-(9,9-dioctylfluorene)-alt-4,7-bis(thiophen-2-yl)benzo-2,1,3-thiadiazole] (PFO-DBT) nanorod bundles. The morphological, structural, and optical properties of PFO-DBT nanorod bundles are enhanced by varying the spin coating rate (100, 500, and 1,000 rpm) of the common spin coater. The denser morphological d...

Journal: :Science and technology of advanced materials 2011
Agnieszka Kurek Seán T Barry

We report an accessible and simple method of producing 'black silicon' with aspect ratios as high as 8 using common laboratory equipment. Gold was sputtered to a thickness of 8 nm using a low-vacuum sputter coater. The structures were etched into silicon substrates using an aqueous H2O2/HF solution, and the gold was then removed using aqua regia. Ultrasonication was necessary to produce columna...

Journal: :Journal of the Society of Powder Technology, Japan 1986

1998
R. R. Willey

We have found that the deposition of critical optical thin film stacks with silicon dioxide from an electron beam gun is severely limited by the stabilty of the evaporation pattern of the material. We had not obtained satisfactory results in some of the more demanding applications with either solid or granular starting material. The amount of material deposited on a central monitor chip or cont...

نمودار تعداد نتایج جستجو در هر سال

با کلیک روی نمودار نتایج را به سال انتشار فیلتر کنید