2017
K. Anandan V. Rajendran

Chromia (Cr2O3) nanoparticles have been successfully synthesized via the facile solvothermal process, by using CrO3 in butanol and propanol as solvents. The functional groups of the samples were tested by the Fourier Transform Infrared (FTIR) spectroscopy. The as-synthesized nanoparticle sizes are calculated and confirmed to be 34 and 40 nm, by using X-ray Diffraction (XRD) and Transmission Ele...

Journal: :Advanced Functional Materials 2022

Focused-Ion-Beam Machining Sacrificial masking films enable focused-ion-beam machining of complex nanostructures beyond the resolution limit ion beam, but current understanding this super-resolution effect is both empirical and spatial. In article number 2111840, Samuel M. Stavis co-workers introduce chromia as a multifuntional material develop new theory that elucidates resolution–throughput t...

Journal: :MATEC web of conferences 2021

Cr2O3 and TiO2 powders were deposited by atmospheric plasma spray (APS) on steel substrates. Microstructural analysis of the coatings showed typical lamellar structure with good coating quality. Fatigue strength was studied using cyclic testing (measuring an inhouse-built apparatus coated systems under a wide range impact cycles) static loading tests (Vickers standards 600N 1500N) measuring adh...

Journal: :Nanotechnology 2009
J B Bult W G Sawyer P M Ajayan L S Schadler

Vertically aligned arrays of multi-wall carbon nanotubes (MWNT) are grown on Inconel 600, a nickel-based super-alloy. Using x-ray photoelectron spectroscopy (XPS) and chemical vapor deposition (CVD) growth of the MWNTs it is shown that a stable oxidation barrier is required for the stabilization of iron on the substrate and subsequent nanotube growth. This evidence for passivation oxide support...

In this research the effects of; increasing the amount of nickel and adding aluminum to create and prolong sulfidation resistance of Fe-Ni-Cr alloys have been investigated. Sulfidation tests were carried out at 1100°C in S/O bearing atmosphere. Prior to the tests, the specimens were annealed in argon at 1250°C for 8 hrs. Weight changes were measured and corroded deposits were analyzed byscannin...