INTRODUCTION In lingual orthodontic therapy, effective torque control of the incisors is crucial due to the biomechanical particularities associated with the point of force application and the tight link between third order deviations and vertical tooth position. AIM The aim of the present in vitro investigation was to analyze the torque capacity of a completely customized lingual appliance o...
BACKGROUND The aim of this study is to investigate the relative stiffness of straight and mushroom lingual archwires of different diameters, cross sections and alloys, plotting their load/deflection graphs and using a modified three-point bending test. METHODS Fujita's mushroom archwires and straight lingual archwires of different diameters, cross sections and alloys were derived by a virtual...
OBJECTIVE This study evaluated in vitro the mechanical changes of 0.018" (0.45 mm) and 0.016 × 0.022" (0.40 × 0.55 mm) thermoactivated nickel-titanium archwires subjected to heat treatment on their distal ends. MATERIALS AND METHODS Ten archwires in diameters 0.018" and 0.016 × 0.022" by different manufacturers Ormco, Morelli, Orthometric and Unitek were tested. Each tested archwire had an ex...
AIM This in vitro study measured the force-deflection behavior of selected initial alignment archwires by conducting three-point bending tests under controlled conditions. The study tested four wire designs: multistranded stainless steel, conventional stainless steel, superelastic nickel-titanium, and thermoactivated nickel-titanium archwires. METHOD The wires (n = 15) were ligated into stain...
OBJECTIVES The aim of this study was to assess and compare the characteristics of commonly used initial archwires by their load deflection graphs. MATERIALS AND METHODS This study tested three wire designs namely copper nickel titanium (CNT), nickel titanium (NiTi), and multi-strand NiTi (MSNT) archwires engaged in passive self-ligating (PSL) brackets, active self-ligating (ASL) brackets or c...
The aim of this study was to evaluate the frictional force between orthodontic brackets and archwires. The differences in magnitude of the frictional forces generated by ceramic brackets, ceramic brackets with metal reinforced slot, and stainless steel brackets in combination with stainless steel, nickel-titanium, and beta-titanium orthodontic archwires were investigated. Brackets and wire were...
BACKGROUND The major hazard to the orthodontic tooth movement is the friction developing at the bracket wire interface. In the past, there have been various attempts to reduce this friction. We believe that coating the commercially available orthodontic wires with nanoparticles can result in a successful reduction of this friction. The objective of this study is to develop a novel method of coa...
The purpose of the study was to measure and compare the level of frictional resistance generated between conventional ceramic brackets (Transcend Series 6000, 3M Unitek, Monrovia, Calif), ceramic brackets with stainless steel slot (Clarity, 3M Unitek), conventional stainless steel brackets (Victory Series, 3M Unitek), and 3 different orthodontic wire alloys: stainless steel (stainless steel, SD...
OBJECTIVE To evaluate the color stability of six esthetic archwires at different time periods and their fluorescence. MATERIALS AND METHODS Samples were evaluated after 7, 14, and 21 days of immersion in staining solution. Color measurements were performed by means of a spectrophotometer according to the Commission Internationale de I'Eclairage L*a*b* system, and color changes (ΔE*) and Natio...